LAIRD TPUTTY 607

Harmonization Code : 8547.90.00.00 | Insulating fittings for electrical machines, appliances or equipment, being fittings wholly of insulating material apart from any minor components of metal (for example, threaded sockets) incorporated during moulding solely for purposes of assembly, other than insulators of heading 8546; electrical conduit tubing and joints therefor, of base metal

LAIRD TPUTTY 607

Main features

  • 6.4 W/(m K) Thermal Interface
  • No-Mix Thermal Interface Processing
  • Automation-Oriented Dispensing and Vertical Stability

Product Description

Laird™ Tputty™ 607 is a blue, silicone-based, single-part dispensable thermal gap filler developed for automated application and vertical stability. The ready-to-use material requires no mixing or post-cure and adapts to variable interface gaps while maintaining contact between heat-generating components and cooling hardware. Tputty 607 provides a typical thermal conductivity of 6.4 W/m·K, supports a minimum bondline thickness of 0.15 mm, and operates from -40 to 200 °C. Its dispensable format is available in multiple cartridge and bulk-packaging options for prototype through high-volume production.

Key features

  • High thermal conductivity: Provides a typical thermal conductivity of 6.4 W/m·K for heat transfer across component-to-cooling interfaces.
  • Ready-to-use single-part material: Requires no component mixing or post-cure before installation.
  • Automation and vertical stability: Supports dispensing in automated production and installation in different application orientations.

Applications / Suitable for

  • Automotive electronics
  • Servers and wireless infrastructure
  • Gaming systems and smart-home devices
  • Notebooks, tablets, and portable devices
  • Drones and satellites

Technical Specifications

General Properties
Color
The color
Blue
Density (g)
3.45 g/cm3
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
6.4 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties and handling conditions for the single-part material before dispensing and installation.

Property Value Unit Method / condition
Product form Single-part dispensable material — Ready to use; mixing and post-cure are not required
Color Blue — As supplied
Density 3.50 g/cc Typical value; test method not stated
Shelf life 6 months From date of manufacture
Recommended storage temperature 0 to 35 °C Store in original packaging; cartridges stored vertically in tip-down dispensing orientation
Technical properties

After-processing / final-state properties

Typical properties relevant to Tputty 607 after dispensing and installation as a thermal interface. The product does not require post-cure.

Property Value Unit Method / condition
Thermal conductivity 6.40 W/m·K Typical bulk-material value; test method and conditions not stated
Minimum bondline thickness 0.15 mm Equivalent to 150 µm
Operating temperature range -40 to 200 °C Retention of individual properties across the full range is not stated
Dielectric constant 15.00 — Test frequency and method not stated
Volume resistivity 1.00 × 1013 Ω·cm Test method and conditioning not stated
Total mass loss 0.204 % TML, ASTM E595
Collected volatile condensable material 0.010 % CVCM, ASTM E595