TEROSON MS 5570

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

TEROSON MS 5570

Main features

  • One-Component Moisture-Cure Polymer
  • Fast Skin-Over Processing
  • Elastic Structural Bonding

Product Description

TEROSON® MS 5570™ is a one-component, moisture-curing modified silane polymer adhesive and sealant for elastic bonding and sealing across a variety of substrates. The white paste cures through exposure to atmospheric moisture to form an elastomeric thermoset material. It combines high strength, high elongation, high initial tack, sag resistance, good UV resistance, and compatibility with suitable paint systems for interior and exterior applications.

Key features

  • Elastic bonding and sealing: Provides a high-strength, flexible bond with 230% elongation at break.
  • One-component moisture cure: Requires no mixing, develops functional strength in approximately 24 hours, and fully cures in about seven days under normal conditions.
  • Broad application performance: Offers high initial tack, sag resistance, good UV resistance, and compatibility with suitable paint systems.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White paste
Density (g)
1.28 - 1.44 g/cm3
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
230 %
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
-64 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Flextec™ polymer — Uncured material
Chemical type Modified silane polymer — Uncured material
Appearance White paste — Uncured material
Components One component — No mixing required
Density 1.28–1.44 g/mL ISO 2811-1; 22°C
Extrusion rate 200–900 g/min Typical uncured-material property
Flow 0–3 mm ISO 7390
Skin-over time 10–60 min 25 ± 2°C, 50 ± 5% RH
Depth of cure 1–6 mm/day Moisture-cure rate; depends on temperature and humidity
Flash point 96 °C ASTM D3278, Setaflash closed cup; SDS value
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on the stated cure schedule, substrate, specimen, and test method.

Property Value Unit Method / condition
Service temperature −30 to 80 °C Continuous service range
Maximum intermittent exposure temperature 100 °C Intermittent exposure
Elongation at break 230 % ISO 527-3; cured 21 days at 22°C and 50 ± 5% RH
Tensile strength 2.4 N/mm² ISO 527-3; cured 21 days at 22°C and 50 ± 5% RH
Glass-transition temperature −64 °C ISO 11357-2; cured 21 days at 22°C and 50 ± 5% RH
Nonvolatile content 98 % ASTM D2369; cured 21 days at 22°C and 50 ± 5% RH
Shore hardness 53 Shore A ISO 868; cured 21 days at 22°C and 50 ± 5% RH
Lap-shear strength 2.8 N/mm² ISO 4587; grit-blasted steel; cured 21 days at 22°C
Lap-shear strength 2.6 N/mm² ISO 4587; glass; cured 21 days at 22°C
Block-shear strength 3.2 N/mm² ISO 13445; nylon; cured 21 days at 22°C
T-peel strength 0.5 N/mm ISO 11339; aluminum; cured 21 days at 22°C
Impact strength 3.4 J ISO 9653; aluminum; cured 21 days at 22°C