Techsil TIM11150 (GB)

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Techsil TIM11150 (GB)20oz

Main features

  • 2.30 W/(m K) Thermal Conductivity
  • Embedded 50 um Glass Beads
  • Non-Corrosive Bonding Formulation

Product Description

Techsil® TIM11150 (GB) is a one-part, solvent-free acetone-cure RTV silicone sealant containing 50 µm glass beads for controlled self-gapping applications. The grey paste cures through atmospheric moisture to form a tough elastomer and is non-corrosive to copper and copper alloys. It combines fast skin formation with a typical cured thermal conductivity of 2.30 W/m·K and documented electrical insulation properties.

Key features

  • Thermally conductive cured elastomer: Provides a typical thermal conductivity of 2.30 W/m·K after seven days of cure at 23 ± 2 °C and 65% relative humidity.
  • Controlled self-gapping: Contains 50 µm glass beads to maintain separation in supported self-gapping applications.
  • Non-corrosive moisture cure: The one-part, solvent-free acetone-cure system does not corrode copper or copper alloys and reaches tack-free condition in four minutes under stated conditions.

Applications / Suitable for

  • Self-gapping applications requiring 50 µm glass-bead spacing
  • Sealing and adhesive applications where a one-part RTV silicone is suitable
  • Applications involving copper or copper-alloy surfaces where non-corrosive cure is required
Product Family

TECHSIL TIM11150GB

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
gray paste
Color
The color
gray
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.11
Physical Properties
Tack-Free Time
4 minutes
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
350,000 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
103 %
Thermal Properties
Operating Temperature
-50 to 220 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
2.30 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and processing properties of Techsil® TIM11150 (GB). Typical technical data are not intended for specification purposes.

Property Value Unit Method / condition
Chemistry and cure type One-part, acetone-cure RTV silicone — Moisture cure; solvent free
Color and appearance Grey paste — As supplied
Glass-bead particle size 50 µm For self-gapping applications
Viscosity 350,000 mPa·s Brookfield
Tack-free time 4 minutes Measured at 23 ± 2 °C and 65% relative humidity
Cure-through time <8 hours 3 mm section at 23 ± 2 °C and 65% relative humidity
Full cure 7 days Supplier-stated full-cure time
Shelf life 12 months Expected in original unopened containers stored below 40 °C
Technical properties

After-processing / final-state properties

Typical cured properties of Techsil® TIM11150 (GB) after seven days at 23 ± 2 °C and 65% relative humidity, except where otherwise stated. Typical technical data are not intended for specification purposes.

Property Value Unit Method / condition
Tensile strength 3.90 MPa BS 903 Part A2
Elongation at break 103 % BS 903 Part A2
Hardness 67 Shore A ASTM D2240-95
Specific gravity 2.11 — BS 903 Part A1
Linear shrinkage 0.5 % Test method not stated
Thermal conductivity 2.30 W/m·K Test method not stated
Service temperature -50 to 220 °C Minimum stated without method; maximum per AFS 1540B
Volume resistivity 1 × 1014 Ω·cm ASTM D257
Dielectric strength 20 kV/mm ASTM D149