LOCTITE STYCAST US 2350

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE STYCAST US 2350

Main features

  • Flame retardent
  • Low CTE
  • Room temperature curing

Product Description

LOCTITE STYCAST US 2350 is a flexible, flame retardant, mineral-filled, polyurethane compound. This potting compound has long pot life, and is low viscosity so it flows well and adheres to many substrates. It has very low odor and does not contain TDI or mercury compounds.

LOCTITE STYCAST US 2350 has a mixing ratio 1:4 by volume and cures at room temperature. 

Product Family

STYCAST US 2350

1. Select Package Type

Loading pricing…

Product availability
US Shipping in 15 days
CA Shipping in 12 weeks
EU Shipping in 30 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
1.4 g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
21.2:100
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
0.75 hours
Thermal Properties
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V2
Electrical Properties
Surface Resistivity
1540000000000000 Ohms/sq
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
61200000000000 Ohms⋅cm
Chemical Properties
Water Absorption
0.09 %

Additional Information

Recommended Curing Conditions

  • 12 to 24 hours @ 23 °C


Alternate Cure Schedule

  • 1 to 3 hours @ 65 to 85°C

Leading Brands Trust in Our Products and Services