Loctite STYCAST 3103

Harmonization Code : 3907.30.00.15 | Epoxide resin, halogen-free

Loctite STYCAST 3103

Main features

  • Low-Viscosity Solvent-Free Epoxy
  • Room-Temperature or Heat Cure
  • Electrically Insulating Epoxy

Product Description

LOCTITE® STYCAST 3103 BIPAX is a black, two-part, solvent-free epoxy casting compound for potting and encapsulation applications requiring mechanical, thermal, and electrical insulating properties. The low-viscosity system mixes at a 100:10.5 resin-to-hardener ratio by weight and can be cured at room temperature or with heat. Once cured, it provides resistance to thermal shock, impact, chemicals, and environmental exposure across an operating temperature range of -60 to 145°C.

Key features

  • Electrical insulation: Formulated for applications requiring electrically insulating encapsulation.
  • Low-viscosity processing: Provides a mixed viscosity of 4,000 mPa·s (cP) at 25°C for casting and potting.
  • Flexible cure options: Cures in 24 hours at 25°C or 4 hours at 65°C.
  • Durable cured performance: Resists thermal shock, impact, chemicals, and environmental exposure.
  • Low-outgassing and cytotoxicity testing: Passes NASA outgassing standards and ISO 10993-5 elution cytotoxicity testing.

Applications / Suitable for

  • Potting and encapsulation
  • Applications requiring mechanical, thermal, and electrical insulating properties
  • Use with glass, ceramic, most metals, potting shells, and other plastics

Technical Specifications

General Properties
Color
The color
black
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
two part
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100 : 10.5
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
80 °C
Operating Temperature
-60 to 145 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
5×10^-1 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
4×10^16 Ohms⋅cm

Additional Information

Technical properties

After-processing / final-state properties

Typical cured properties. Values are not intended for use as specifications.

Property Value Unit Method / condition
Operating temperature -60 to 145 °C Cured material
Coefficient of thermal expansion 3.5 × 10-5 cm/cm/°C Typical cured property
Glass transition temperature (Tg) 80 °C Ultimate
Hardness 85 Shore D Typical cured property
Reactive solids content 100 % Typical cured property
Thermal conductivity 5 × 10-1 W/(m·K) Typical cured property
Heat distortion temperature 102 °C Typical cured property
Volume resistivity 4 × 1016 ohm·cm At 25°C
Volume resistivity 4 × 1014 ohm·cm At 100°C
Dielectric strength 510 volts/mil Typical cured property
Dielectric constant / dissipation factor 4.1 / 0.01 — At 25°C and 1 kHz
Dielectric constant / dissipation factor 3.8 / 0.01 — At 25°C and 100 kHz
Lap shear strength, aluminum to aluminum 18 (2,600) N/mm² (psi) Typical cured performance