STYCAST 2741LV

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

STYCAST 2741LV

Main features

  • Lower-Viscosity Electronic Potting
  • Selectable Rigid-to-Flexible Cure
  • Impact-Resistant Multi-Substrate Encapsulation

Product Description

LOCTITE STYCAST 2741LV Epoxy Encapsulant is a lower-viscosity, black filled epoxy system used with Catalyst 15 LV for electronic embedment, sealing, and cementing of glass, metals, plastics, and ceramics. Changing the catalyst amount produces rigid, semi-rigid, or flexible cured states, while typical mixed viscosity ranges from 16,000 to 30,000 mPa s. Work life is 90 to 120 minutes at 25 deg C, followed by room-temperature or accelerated cure. The cured formulations provide distinct hardness and strength levels with shock and impact resistance for assemblies requiring adjustable mechanical response.

Key features

  • Lower-viscosity processing: Mixed viscosity ranges from 16,000 to 30,000 mPa s across the three formulations.
  • Selectable cured response: Catalyst 15 LV loading produces rigid, semi-rigid, or flexible material.
  • Shock and impact resistance: The product is positioned for assemblies requiring shock or impact resistance.

Applications

Applications include electronic embedment and sealing or cementing of metals, ceramics, and plastics where lower viscosity and adjustable flexibility are useful.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
black
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for STYCAST 2741 LV with Catalyst 15 LV; formulation ratios determine rigid, semi-rigid, or flexible behavior.

Property Value Unit Method / condition
Resin density 1.58 g/cm^3 TP-13
Resin viscosity 35,000 mPa s (cP) TP-10 or TP-11
Catalyst density 0.97 g/cm^3 TP-13
Catalyst viscosity 11,000 mPa s (cP) TP-10 or TP-11
Mixed viscosity 30,000 / 25,000 / 16,000 mPa s (cP) Rigid / semi-rigid / flexible formulations
Work life 120 / 90 / 90 minutes 100 g at 25 deg C; rigid / semi-rigid / flexible
Cure schedule 16 to 24 h at 25 deg C; 4 to 6 h at 45 deg C; 2 to 4 h at 65 deg C; 30 to 60 min at 90 deg C Typical alternatives
Technical properties

After-processing / final-state properties

Typical after-application properties vary with the rigid, semi-rigid, or flexible formulation.

Property Value Unit Method / condition
Hardness 82 Shore D / 74 Shore D / 50 Shore D Rigid / semi-rigid / flexible; TP-311
Compressive strength 98 / 69 / 35 N/mm^2 Rigid / semi-rigid / flexible; TP-207
Tensile strength 48 / 44 / 4 N/mm^2 Rigid / semi-rigid / flexible; TP-239
Glass transition temperature 68 / 38 / 21 deg C Rigid / semi-rigid / flexible; DSC/TMA
Operating temperature range -40 to 90 / -55 to 80 / -55 to 65 deg C Rigid / semi-rigid / flexible
Dielectric strength 16 kV/mm All three formulations; TP-297
Volume resistivity >1 x 10^15 / >1 x 10^15 / >1 x 10^14 ohm cm Rigid / semi-rigid / flexible at 25 deg C; TP-183
Linear shrinkage 0.001 cm/cm All three formulations; TP-320