STYCAST 2662

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

STYCAST 2662

Main features

  • High-Temperature 230 deg C Service
  • Extended 24-Hour Working Window
  • Staged Large-Casting Cure

Product Description

LOCTITE STYCAST 2662 High-Temperature Epoxy Encapsulant is a black, heat-cure epoxy potting system used with CAT 17 for electronics and large or complex castings exposed to elevated temperature, chemicals, and moisture. The 100:30 by-weight mix provides more than 24 hours of work life at 25 deg C, allowing extended preparation and casting time. Regular and staged cure profiles address standard and critical casting geometries. After cure, the material has a -20 to 230 deg C operating range, Shore D 88 hardness, low 24-hour water absorption, and electrical insulation properties.

Key features

  • High-temperature cured service: The CAT 17 system has an operating range of -20 to 230 deg C.
  • Extended work life: The 100 g mixture remains workable for more than 24 hours at 25 deg C.
  • Large-casting cure profile: A staged schedule is provided for larger or critical castings.

Applications

Applications include potting electronic components exposed to harsh environments and encapsulating large or complex castings requiring high-temperature, chemical, and moisture resistance.

Technical Specifications

General Properties
Chemistry Type
epoxy
Color
The color
black
Density (g)
1.44 g/cm3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
40,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and mixed values for STYCAST 2662 with CAT 17.

Property Value Unit Method / condition
Resin appearance Black STYCAST 2662, as supplied
Resin viscosity 40,000 mPa s (cP) Brookfield; typical
Resin density 1.44 g/cm^3 Typical
Mix ratio by weight 100:30 STYCAST 2662:CAT 17
Mixed density 1.41 g/cm^3 Typical
Work life >24 hours 100 g at 25 deg C
Cure schedule Regular: 3 h at 125 deg C plus 3 h at 175 deg C; large or critical: 16 h at 65 deg C plus 6 h at 125 deg C plus 6 h at 150 deg C Guideline alternatives
Technical properties

After-processing / final-state properties

Typical cured properties for the CAT 17 configuration.

Property Value Unit Method / condition
Operating temperature range -20 to 230 deg C CAT 17 cured system
Hardness 88 Shore D Typical cured value
Coefficient of thermal expansion 47 10^-6/deg C Typical cured value
Thermal conductivity 0.53 W/(m K) Typical cured value
Water absorption 0.01 % 24 hours
Dielectric strength 16.5 kV/mm Typical cured value
Volume resistivity >1 x 10^16 ohm cm 25 deg C
Flexural strength 100 N/mm^2 Typical cured value