STYCAST 1495K

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

STYCAST 1495K

Main features

  • Thermally Conductive Electronic Potting
  • 45-Minute CAT 9 Work Life
  • Transformer and Sensor Encapsulation

Product Description

LOCTITE STYCAST 1495K Thermally Conductive Epoxy Encapsulant is a black, filled epoxy encapsulant for electronic components that require a thermally conductive potting material. With CAT 9, the resin mixes 100:4.5 by weight, reaches a typical mixed viscosity of 21,000 cP, and provides a 45-minute working time at 25 deg C. The cured material has a typical thermal conductivity of 1.1 W/(m K), 95 Shore D hardness, electrical insulation, and an operating range of -40 to 130 deg C. Documented applications include transformers, sensors, and related electronic assemblies.

Key features

  • Thermally conductive potting: Typical cured thermal conductivity is 1.1 W/(m K).
  • Controlled CAT 9 processing: The CAT 9 formulation provides a 45-minute working time at 25 deg C.
  • Electrical encapsulation: The cured material combines thermal conduction with dielectric performance.

Applications

Applications include potting of transformers, sensors, and electronic assemblies requiring a thermally conductive, electrically insulating encapsulant.

Product Family

STYCAST 1495K

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black liquid
Density (g)
1.90 g/cm3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
45,000 mPa.s
Other Properties
Storage Temperature
25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

The table uses the CAT 9 formulation; other approved catalysts have different ratios, viscosities, work lives, and cure schedules.

Property Value Unit Method / condition
Product form Black filled epoxy resin Values below use CAT 9 catalyst
Resin viscosity 45,000 cP Brookfield, spindle 6, 10 rpm
Resin specific gravity 1.9 Typical as supplied
Mix ratio 100:4.5 parts by weight Resin:CAT 9
Mix ratio 100:8.5 parts by volume Resin:CAT 9
Mixed viscosity 21,000 cP CAT 9; typical
Mixed specific gravity 1.89 CAT 9; typical
Working time 45 minutes CAT 9 at 25 deg C
Technical properties

After-processing / final-state properties

Typical cured properties for the CAT 9 formulation.

Property Value Unit Method / condition
Thermal conductivity 1.1 W/(m K) CAT 9 cured formulation
Operating temperature -40 to 130 deg C CAT 9 cured formulation
Hardness 95 Shore D CAT 9 cured formulation
Linear shrinkage 0.001 cm/cm CAT 9 cured formulation
Water absorption 0.07 % 24 hours; CAT 9 cured formulation
Coefficient of thermal expansion 42 ppm/deg C CAT 9 cured formulation
Dielectric strength 15.7 kV/mm CAT 9 cured formulation
Volume resistivity 5 x 10^13 ohm cm 25 deg C; CAT 9 cured formulation