STYCAST 1265

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

STYCAST 1265

Main features

  • Soft-Gel Stress-Sensitive Encapsulation
  • Extended 24-Hour Work Life
  • Cuttable Repair Access

Product Description

LOCTITE STYCAST 1265 Epoxy Encapsulant is a clear, two-component epoxy system that cures to a soft gel for encapsulating stress-sensitive electrical and electronic components. The 100:100 by-weight mix has a typical mixed viscosity of 600 cP, a specific gravity of 1.08, and more than 24 hours of working life at 25 deg C. Its low-exotherm cure can proceed at room temperature or with heat, while the final 25 Shore A material remains cuttable for repair access and repouring. The nonconductive gel supports inspection, protection, and re-entry in delicate assemblies.

Key features

  • Soft-gel encapsulation: The cured material has a typical hardness of 25 Shore A.
  • Extended working time: More than 24 hours of work life supports controlled filling and assembly.
  • Repair-accessible protection: The cured gel can be cut and repoured for inspection or repair.

Applications

Applications include encapsulation of stress-sensitive electrical and electronic components requiring a soft, nonconductive gel and later repair access.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two Part (Resin | Hardener)
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
10¹² Ohms⋅cm
Other Properties
Storage Temperature
25 °C
Thermal Properties
Operating Temperature
-40 to 90 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Product form Two-component clear epoxy system Part A and Part B
Mix ratio 100:100 parts by weight Part A:Part B
Part A viscosity 10,000 cP 25 deg C; typical
Part B viscosity 230 cP 25 deg C; typical
Mixed viscosity 600 cP 25 deg C; typical
Mixed specific gravity 1.08 25 deg C; typical
Working life >24 hours 100 g mass at 25 deg C
Cure schedule 3-7 d at 25 deg C; 48 h at 45 deg C; 16 h at 65 deg C; 4 h at 95 deg C Typical options
Technical properties

After-processing / final-state properties

Property Value Unit Method / condition
Operating temperature -40 to 90 deg C Cured material
Hardness 25 Shore A Typical cured value
Volume resistivity 1 x 10^12 ohm cm 25 deg C
Dielectric constant 3.0 1 MHz
Dissipation factor 0.02 1 MHz