STYCAST 1090

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

STYCAST 1090

Main features

  • Low-Density Aerospace Encapsulation
  • 45-Minute Working Window
  • NASA Outgassing Performance

Product Description

LOCTITE STYCAST 1090 Epoxy Encapsulant is a two-component, black syntactic epoxy system for low-density encapsulation and potting. Used with CAT 9 catalyst at 100:9 by weight, the mixed material has a typical specific gravity of 0.79 and a 45-minute working time at 25 deg C. Multiple ambient and heat-cure schedules support production flexibility, while the cured material provides electrical insulation, compressive strength, and service from -40 to 130 deg C. Documented NASA outgassing results support evaluation for aerospace and other weight-sensitive electronic assemblies.

Key features

  • Low-density syntactic formulation: A mixed specific gravity of 0.79 supports lightweight encapsulation.
  • Controlled processing window: CAT 9 provides a typical 45-minute working time at 25 deg C.
  • Documented outgassing data: Typical TML and CVCM values support aerospace material evaluation.

Applications

Applications include low-density encapsulation of aerospace, electronic, and electrical assemblies where weight, insulation, and compressive performance are important.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black Liquid
Density (g)
0.85 g/cm3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
135,000 mPa.s
Other Properties
Storage Temperature
25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Product form Two-component black syntactic epoxy system Resin with CAT 9 catalyst
Mix ratio 100:9 parts by weight Resin:CAT 9
Mix ratio 100:7 parts by volume Resin:CAT 9
Resin viscosity 135,000 cP 25 deg C; Brookfield, spindle 7, speed 10
Mixed viscosity 30,000 cP 25 deg C; typical
Mixed specific gravity 0.79 25 deg C; typical
Working time 45 minutes 100 g mass at 25 deg C
Cure schedule 16-24 h at 25 deg C; 4-6 h at 45 deg C; 1-2 h at 65 deg C CAT 9 formulation
Technical properties

After-processing / final-state properties

Property Value Unit Method / condition
Operating temperature -40 to 130 deg C Cured material
Hardness 80 Shore D Typical cured value
Thermal conductivity 0.19 W/(m K) Typical cured value
Water absorption 0.55 % 24 hours
Compressive strength 12,000 psi Typical cured value
Volume resistivity >1 x 10^13 ohm cm 25 deg C
Total mass loss 0.46 % NASA outgassing test
Collected volatile condensable material 0.06 % NASA outgassing test