SILASTIC RTV-3120

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

SILASTIC RTV-3120

Main features

  • 28,000 cP Base Viscosity
  • High-Temperature Mold Service
  • Adjustable Catalyst-Controlled Cure

Product Description

SILASTIC RTV-3120 Mold-Making Base is a red, high-temperature condensation-cure silicone base for producing molds within a documented catalyst and cure system. The base has a typical viscosity of 280 poise (28,000 cP) and a specific gravity of 1.45 at 25 deg C, supporting pourable processing and reproduction of intricate details. A compatible catalyst is selected and added separately; the base alone does not represent the cured mold rubber or its final performance. Use is limited to validated mold geometry, catalyst ratio, release practice, cure schedule, casting material, and service conditions.

Key features

  • 28,000 cP base viscosity: Supports pourable mold preparation at 25 deg C
  • High-temperature mold base: Supports high-temperature mold-making formulations with the documented catalyst
  • Separate catalyst control: Catalyst selection and ratio establish the working and cure profile

Applications

High-temperature silicone mold making within validated mold geometry, catalyst ratio, release practice, cure schedule, and casting conditions.

Product Family

SILASTIC RTV-3120

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Red
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.45
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
280 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
128 %

Additional Information

Technical properties

As-supplied / before-processing properties

The page entity is the mold-making base only; catalyst selection and cure conditions remain system-dependent.

Property Value Unit Method / condition
Color Red As supplied
Viscosity 280 (28,000) poise (cP) At 25 deg C
Specific gravity 1.45 At 25 deg C
Reference mix ratio 10:1 base:catalyst by weight RTV-3010-S Catalyst reference formulation; catalyst sold separately

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers