SILASTIC 3-8186

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

DOWSIL 3-8186

Main features

  • Low-Force Elastomeric Foam for Dispensed-in-Place Compression Gasketing
  • Reduced-Flow Robotic Bead Dispensing
  • 10-Minute 75 deg C Cure

Product Description

SILASTIC™ 3-8186 Thixotropic Foam is a two-part, platinum-cure liquid silicone foam for dispensed-in-place compression gaskets requiring low sealing force. Parts A and B are mixed at a 1:1 ratio by weight, then expand and cure into a medium-density elastomeric foam with moderate heat. Its thixotropic, reduced-flow behavior supports controlled bead placement using robotic or other automated dispensing equipment. The product is intended for sealing automotive components and lighting assemblies and may also be used for outdoor electrical enclosures.

Key features

  • Low sealing force: Forms compressible foam gaskets for applications where lower compression force is required.
  • Reduced-flow rheology: Supports controlled dispensing and uniform bead placement in automated gasketing processes.
  • Low-temperature heat cure: Expands and cures in approximately 10 minutes at 75°C when properly mixed.

Applications / Suitable for

  • Dispensed-in-place compression gaskets
  • Automotive component sealing
  • Lighting assembly sealing
  • Outdoor electrical enclosure sealing
Product Family

SILASTIC 3-8186

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black / Off white
Density
Volumetric mass per unit
225 kg/m3
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.12 / 1.22
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
140 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the separate components and the mixed material. These values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Color Part A: Black
Part B: Off-white
— CTM 0063; as supplied
Specific gravity Part A: 1.12
Part B: 1.22
— CTM 0044; as supplied
Viscosity Part A: 135,000
Part B: 125,000
cP CTM 0050; as supplied
Mix ratio 1:1 By weight Part A to Part B
Mixed color Black — CTM 0063; 1:1 mix ratio by weight
Snap time 3.5 min CTM 0092A; 1:1 mix ratio by weight
Flow, maximum 4 in CTM 0062; 1:1 mix ratio by weight
Working time Approximately 1 min At 23°C and 50% relative humidity; higher temperatures reduce working time

After-processing / final-state properties

Typical physical properties after curing for 10 minutes at 75°C and equilibrating for 24 hours at 23°C and 50% relative humidity. These values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Foam density 225 (14) kg/m³ (pcf) CTM 0854A
Tensile strength 0.18 (26) MPa (psi) ASTM D412, Die A
Elongation 140 % ASTM D412
Compression deflection, 25% ILD 0.032 (4.7) MPa (psi) CTM 0525 at 23°C
Compression deflection, 50% ILD 0.085 (12.4) MPa (psi) CTM 0525 at 23°C
Compression deflection, 75% ILD 0.33 (48.6) MPa (psi) CTM 0525 at 23°C