SIKAFLEX P2G

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

SIKAFLEX P2G

Main features

  • Primerless Automotive Glass Installation
  • 15-Minute Open Time
  • 5 MPa Tensile Strength

Product Description

Sikaflex P2G is a one-component, cold-applied polyurethane adhesive for direct-glazed automotive glass replacement. The black, high-viscosity material is primerless to glass when used within the documented Sika preparation process and provides a 15-minute open time at 23 deg C and 50% relative humidity. After cure, typical properties include 5 MPa tensile strength, 400% elongation, and 3 MPa tensile lap-shear strength. It is intended for professional mobile and in-shop windshield installation, with bead geometry, substrate preparation, environmental conditions, and vehicle-specific process controls maintained throughout the replacement procedure.

Key features

  • Primerless-to-glass process: Supports direct glazing when the documented Sika preparation procedure is followed
  • 15-minute open time: Defines the glass-installation window at 23 deg C and 50% relative humidity
  • Cold-applied high viscosity: Provides excellent non-sag behavior for triangular bead placement

Applications

Professional automotive replacement glazing and windshield bonding for mobile and in-shop installation under the documented Sika process controls.

Product Family

SIKAFLEX P2G

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
polyurethane
Color
The color
black
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
one
Density
Volumetric mass per unit
1.3 kg/m3
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
400 %
Thermal Properties
Operating Temperature
-40 to 93 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Chemical base 1-component polyurethane As supplied
Color Black CQP001-1
Density 1.3 kg/l Uncured
Non-sag behavior Excellent As supplied
Product application temperature 10 to 35 deg C Adhesive temperature
Ambient application temperature 4 to 43 deg C Installation environment
Substrate application temperature 4 to 54 deg C Bonding surface
Skin time 30 minutes CQP019-1; 23 deg C / 50% RH
Open time 15 minutes CQP526-1; 23 deg C / 50% RH
Shelf life 9 months Storage below 25 deg C
Technical properties

After-processing / final-state properties

Property Value Unit Method / condition
Hardness 65 Shore A CQP023-1 / ISO 48-4
Tensile strength 5 MPa CQP036-1 / ISO 527
Elongation at break 400 % CQP036-1 / ISO 527
Tensile lap-shear strength 3 MPa CQP046-1 / ISO 4587
Service temperature -40 to 93 deg C CQP509-1 / CQP513-1