SIKAFLEX 268

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

SIKAFLEX 268

Main features

  • Accelerated Cure Process Option
  • Rail Cleaning-Agent Resistance
  • Exterior Rail Glazing and Assembly

Product Description

Sikaflex-268 is a one-component, moisture-curing polyurethane adhesive and sealant for rail assembly, direct glazing, and repair bonding. It can be processed conventionally or accelerated with Sika Booster and PowerCure systems, while the non-sag material provides a 40-minute open time at 23 deg C and 50% relative humidity. The cured material has 6 MPa tensile strength, 500% elongation, and 4.5 MPa tensile lap-shear strength under ISO 527 and ISO 4587. Its weathering stability and resistance to specified rail cleaning agents support exterior rail joints when dilution, exposure time, and rinsing follow the cleaning-agent guidance.

Key features

  • Accelerated cure option: Processing can be accelerated with Sika Booster and PowerCure systems
  • Rail cleaning-agent resistance: Resistance applies when dilution, exposure time, and rinsing follow the product guidance
  • Exterior rail performance: Weathering stability supports assembly and glazing in exterior rail joints

Applications

Rail and commercial-vehicle assembly; direct glazing; repair bonding; exterior rail joints.

Product Family

SIKAFLEX 268

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
polyurethane
Color
The color
black
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
one
Density
Volumetric mass per unit
1.3 kg/m3
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
500 %
Thermal Properties
Operating Temperature
-40 to 90 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Chemical base 1-component polyurethane As supplied
Color Black CQP001-1
Density 1.3 kg/l Uncured
Non-sag properties Very good CQP061-1
Application temperature 5 to 40 deg C Product and ambient range
Skin time 60 minutes CQP019-1; 23 deg C / 50% RH
Open time 40 minutes CQP526-1; 23 deg C / 50% RH
Shelf life - unipack 12 months Storage below 25 deg C
Technical properties

After-processing / final-state properties

Property Value Unit Method / condition
Shrinkage 1 % CQP014-1
Hardness 55 Shore A CQP023-1 / ISO 48-4
Tensile strength 6 MPa CQP036-1 / ISO 527
Elongation at break 500 % CQP036-1 / ISO 527
Tear propagation resistance 13 N/mm CQP045-1 / ISO 34
Tensile lap-shear strength 4.5 MPa CQP046-1 / ISO 4587
Service temperature -50 to 90 deg C CQP509-1 / CQP513-1