SIKAFLEX 252

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

SIKAFLEX 252

Main features

  • Dynamic-Stress Assembly Bonding
  • Non-Sag Gap-Filling Application
  • Electrically Non-Conductive Bondline

Product Description

Sikaflex-252 is a one-component, moisture-curing polyurethane assembly adhesive for bonding large components exposed to dynamic stresses. The non-sag material provides good gap-filling behavior and a 35-minute open time at 23 deg C and 50% relative humidity. Its cured profile combines 3 MPa tensile strength, 400% elongation, and 2.5 MPa tensile lap-shear strength under ISO 527 and ISO 4587. The adhesive is electrically non-conductive and vibration-damping and is used on timber, coated metals, aluminum, steel, ceramics, GRP, and plastics in vehicle and industrial assemblies.

Key features

  • Dynamic-stress bonding: The elastic adhesive is used for assemblies exposed to dynamic loads
  • Gap-filling non-sag bead: Good gap-filling and non-sag behavior support controlled application
  • Electrically non-conductive: The adhesive is electrically non-conductive

Applications

Bonding large vehicle and industrial components; assemblies subject to dynamic stresses; coated metals, GRP, ceramics, timber, and plastics.

Product Family

SIKAFLEX 252

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
polyurethane
Color
The color
black,white
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
one
Density
Volumetric mass per unit
1.2 kg/m3
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
400 %
Thermal Properties
Operating Temperature
-40 to 90 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Chemical base 1-component polyurethane As supplied
Color Black, white CQP001-1
Density 1.20 kg/l Uncured; color dependent
Non-sag properties Good As supplied
Application temperature 10 to 35 deg C Product and ambient range
Skin time 40 minutes CQP019-1; 23 deg C / 50% RH
Open time 35 minutes CQP526-1; 23 deg C / 50% RH
Shelf life - cartridge / unipack 9 months Storage below 25 deg C
Technical properties

After-processing / final-state properties

Property Value Unit Method / condition
Hardness 50 Shore A CQP023-1 / ISO 48-4
Tensile strength 3 MPa CQP036-1 / ISO 527
Elongation at break 400 % CQP036-1 / ISO 527
Tear propagation resistance 7 N/mm CQP045-1 / ISO 34
Tensile lap-shear strength 2.5 MPa CQP046-1 / ISO 4587
Service temperature -40 to 90 deg C CQP509-1 / CQP513-1
Short-term temperature 130 deg C 4-hour exposure
Short-term temperature 150 deg C 1-hour exposure