SIKAFAST 3121

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

SIKAFAST 3121

Main features

  • Fast Five-Minute Open Time
  • High-Ductility Structural Bonding
  • Concealed-Joint Fastener Replacement

Product Description

SikaFast-3121 is a fast-curing, two-component methacrylate structural adhesive for high-strength fastening of concealed joints. The 10:1 volume-mix thixotropic paste has a five-minute open time at 23 deg C and develops strength within minutes after application. Its toughened cured profile includes 80% elongation and 10.5 MPa tensile lap-shear strength under ASTM D638 and CQP046-6 / ISO 4587. The adhesive bonds aluminum, stainless steel, galvanized steel, and fiber-reinforced polymers and can replace or complement rivets, screws, or welding in assembly applications. Bond thickness is controlled between 0.5 and 5 mm during application.

Key features

  • Fast strength development: Strength builds within minutes after application
  • Five-minute open time: Defines the assembly window at 23 deg C and 50% relative humidity
  • Toughened structural profile: Typical cured properties include 80% elongation and 10.5 MPa tensile lap-shear strength

Applications

High-strength fastening of concealed joints; bonding aluminum, stainless steel, galvanized steel, and fiber-reinforced polymers; replacing or complementing rivets, screws, or welding.

Technical Specifications

General Properties
Chemistry Type
Methacrylate
Color
The color
Dark Gray, Straw
Density (g)
0.99 g/cm3
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
80 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for SikaFast-3121 Part A, SikaFast-3081 N Part B, and the mixed adhesive system.

Property Value Unit Method / condition
Part A density 0.96 kg/l SikaFast-3121 Part A
Part B density 1.30 kg/l SikaFast-3081 N Part B
Mixed density 0.99 kg/l Calculated mixed value
Mix ratio by volume 10:1 Part A:Part B
Mix ratio by weight 7.4:1 Part A:Part B
Consistency Thixotropic paste Mixed adhesive
Application temperature 10 to 35 deg C Substrate and adhesive range
Open time 5 minutes CQP526-2; 23 deg C / 50% RH
Technical properties

After-processing / final-state properties

Typical cured values for the mixed adhesive system.

Property Value Unit Method / condition
Hardness 65 Shore D CQP023-1 / ISO 48-4
Tensile strength 9 MPa ASTM D638
Elongation at break 80 % ASTM D638
E-modulus at 0-5% elongation 100 MPa ASTM D638
Tensile lap-shear strength 10.5 MPa CQP046-6 / ISO 4587
Service temperature -30 to 80 deg C CQP513-1

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers