Loctite SI 5970 - Gasketing Sealant

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite SI 5970 - Gasketing Sealant

Main features

  • One-Component Thixotropic RTV Silicone
  • 25-Minute Tack-Free Time
  • Oil-Resistant Sheet-Metal Gasketing

Product Description

LOCTITE® SI 5970™ Gasketing Sealant is a one-component, black alkoxy silicone paste developed for formed-in-place gasketing applications. The thixotropic formulation reduces migration after dispensing and cures at room temperature through exposure to atmospheric moisture. It becomes tack-free within 25 minutes at 23±2°C and 50±5% relative humidity. The sealant is specifically designed for applications requiring resistance to automotive engine oils and the ability to accommodate joint movement, including stamped sheet-metal covers such as timing covers and oil sumps.

Key features

  • Thixotropic gasketing paste: Reduced liquid migration supports controlled application to flange and cover surfaces.
  • Room-temperature moisture cure: The one-component system requires no mixing and becomes tack-free within 25 minutes at 23±2°C and 50±5% relative humidity.
  • Automotive oil resistance: Developed for gasketing applications requiring resistance to automotive engine oils and joint movement.

Applications / Suitable for

  • Formed-in-place gasketing applications
  • Stamped sheet-metal covers
  • Timing covers
  • Oil sumps
Product Family

SI5970

Loading pricing…

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
black paste
Chemistry Type
Alkoxy silicone
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.38-1.44
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
200 %
Electrical Properties
Surface Resistivity
1.4×1016 Ohms/sq
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1.8×1015 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of LOCTITE® SI 5970™ before cure. LMS-designated values are controlled under the referenced Loctite Material Specification.

Property Value Unit Method / condition
Chemical type Alkoxy silicone — One-component RTV silicone
Appearance Black paste — Uncured; LMS
Rheology Thixotropic — Reduced migration after application
Specific gravity 1.38–1.44 — At 25°C; LMS
Extrusion rate 40–80 g/min Semco cartridge; 0.62 MPa pressure; 15 seconds; 25°C; LMS
Optimal storage temperature 8–21 °C Store unopened in a dry location; long-term storage
Technical properties

After-processing / final-state properties

Typical properties of the cured sealant and substrate-specific adhesive performance. Lap-shear specimens were cured for 21 days at 23°C and 50±5% relative humidity with a 0.5 mm gap.

Property Value Unit Method / condition
Shore hardness 44 Shore A ISO 868
Elongation ≥200 % ISO 37; LMS
Tensile strength ≥1.5 (≥278) N/mm² (psi) ISO 37; LMS
Surface resistivity 1.4 × 1016 Ω IEC 60093
Volume resistivity 1.8 × 1015 Ω·cm IEC 60093
Tensile lap shear strength on mild steel 1.3–2.0 (190–290) N/mm² (psi) Cured 21 days at 23°C / 50±5% RH; 0.5 mm gap
Tensile lap shear strength on aluminum 2024-T3 0.7–1.3 (100–190) N/mm² (psi) Cured 21 days at 23°C / 50±5% RH; 0.5 mm gap