ROYAL WS-8032S

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

ROYAL WS-8032S

Main features

  • Ultra-lightweight mixed density
  • Two Class B work lives
  • 360 deg F intermittent exposure

Product Description

Royal Sealants WS-8032S Class B Ultra-Lightweight Fast-Cure High-Temperature Sealant is a two-part polysulfide paste for lightweight, fast-cure sealing of aircraft fuel tanks and fuselage structures. The chemically cured Class B system is supplied in B-1/2 and B-2 application-life variants and can be applied by extrusion or spatula spreading. Its low-sag, thixotropic handling supports controlled placement, while the cured material is documented for intermittent exposure up to 360 deg F. The product combines low density with defined cured tensile, elongation, hardness, and low-temperature-flexibility data for aerospace sealant evaluation.

Key features

  • Ultra-lightweight sealant: Uses an approximately 1.15 g/cc mixed density
  • Controlled Class B profiles: Provides 0.5- or 2-hour application life
  • High-temperature exposure: Supports intermittent conditions up to 360 deg F

Applications

Aerospace fuel tank and fuselage sealing where the documented WS-8032S Class B process, substrate, temperature, and qualification scope apply.

Product Family

ROYAL WS-8032S

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black, extrudable paste
Chemistry Type
2-part, ultra-lightweight polysulfide fuel-tank / fuselage sealant
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
≈1.15 (mixed density)

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Product form Paste - As supplied
Appearance Black extrudable - As-supplied appearance
Mixed density Approx. 1.15 g/cc After component mixing
Mix ratio by volume 7.55:100 - Hardener:base
Mix ratio by weight 12:100 - Hardener:base
Mixed viscosity 14,000 to 16,000 poise Mixed material
Application life 0.5 / 2 h Class B-1/2 / Class B-2
Shelf life 9 months Original unopened container below 80 deg F
Technical properties

After processing / final state

Property Value Unit Method / condition
Low-temperature flexibility No loss of adhesion or cracking - At -65 deg F
Intermittent exposure temperature Max. 360 deg F Documented intermittent exposure
Tensile strength 300 psi At 77 deg F after 14-day standard cure
Ultimate elongation 300 % At 140 deg F after 42 days; AMS 2629
Ultimate hardness 52 Shore A Cured material
Nonvolatile content Min. 96 % Cured material
Weight loss 3.65 % AMS 2629 Type I