ROYAL DOUBLE BUBBLE 04023

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ROYAL DOUBLE BUBBLE 04023

Main features

  • Fast Five-Minute Working Window
  • High-Hardness Rigid Urethane Bond
  • Strength with 80% Elongation

Product Description

Hardman Double/Bubble 04023 Urethane D-85 Adhesive is a 3.5 g premeasured, two-part polyurethane structural adhesive packet with a rigid cured profile. The beige mixed adhesive has a viscosity of 11,000 cP at 25 deg C, a 5 minute work time, and a 1 hour handling time. After a 24 hour room-temperature cure, typical properties include 85 Shore D hardness, 3,350 psi tensile strength, 80% elongation, and 4,075 psi lap shear strength on acid-etched aluminum at 25 deg C. The material also reaches 10 pli T-peel strength and has a maximum service temperature of 93 deg C.

Key features

  • Rigid D-85 cured profile: Typical cured hardness is 85 Shore D at 25 deg C.
  • Fast handling profile: A 5 minute work time is followed by 1 hour handling strength.
  • Strength with elongation: Typical tensile strength is 3,350 psi with 80% elongation.

Applications

Applications include bonding engineering thermoplastics, SMC, laminated surfaces, and repair of urethane molded parts, rubber hoses, and flexible electrical connections.

Product Family

ROYAL DOUBLE BUBBLE 04023

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Service temperature
93 °C

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Package size3.5gPremeasured dual-pouch packet
Part A viscosity18,000cPAt 25 deg C
Part B viscosity4,000cPAt 25 deg C
Mixed viscosity11,000cPAt 25 deg C
Mixed specific gravity1.26-At 25 deg C
Work time5minAt room temperature
Handling strength1hAt room temperature
Shelf life12monthsPart A and Part B
Technical properties

After processing / final state

Property Value Unit Method / condition
Hardness85Shore DTested at 25 deg C
Tensile strength3,350psiTested at 25 deg C
Elongation80%Tested at 25 deg C
Tear strength800pliTested at 25 deg C
Maximum service temperature93deg CCured adhesive
Lap shear strength4,075psiAcid-etched aluminum-to-aluminum; 24 h room-temperature cure; tested at 25 deg C
T-peel strength10pliAcid-etched aluminum-to-aluminum; 24 h room-temperature cure; tested at 25 deg C