ROYAL DOUBLE BUBBLE 04008

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

ROYAL DOUBLE BUBBLE 04008

Main features

  • Non-Sag Vertical Bonding Control
  • Fast 15-to-30-Minute Handling
  • 82 deg C Service Capability

Product Description

Hardman Double/Bubble 04008 Non-Sag Extra Fast-Setting Epoxy is a 3.5 g premeasured, two-part epoxy packet with a thixotropic paste consistency for vertical, overhead, and gap-filling work. The opaque-white mixed adhesive resists sag on upright surfaces and provides a 3 minute work time followed by 15 to 30 minute handling strength. Typical uncured component viscosities are 465,000 cP for Part A and 400,000 cP for Part B at 25 deg C. After cure, the material reaches 83 Shore D hardness and a maximum service temperature of 82 deg C. The grade is used for rapid repair, fixturing, tacking, sealing, gap filling, and staking.

Key features

  • Non-sag vertical control: The thixotropic paste remains suited to vertical and overhead application.
  • Fast handling: Handling strength develops in 15 to 30 minutes after a 3 minute work time.
  • Rigid cured profile: Typical final hardness is 83 Shore D at 25 deg C.

Applications

Applications include rapid vertical or overhead repair, fixturing, tacking, sealing, gap filling, and staking on supported wood, glass, metal, stone, ceramic, and leather surfaces.

Product Family

ROYAL DOUBLE BUBBLE 04008

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Service temperature
82 °C

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Package size3.5gPremeasured dual-pouch packet
Mixed colorOpaque white-Mixed adhesive
Part A viscosity465,000cPAt 25 deg C
Part B viscosity400,000cPAt 25 deg C
Mixed consistencyThixotropic paste-At 25 deg C
Work time3minAt room temperature
Handling strength15-30minAt room temperature
Shelf life24monthsPart A and Part B
Technical properties

After processing / final state

Property Value Unit Method / condition
Hardness83Shore DTested at 25 deg C
Maximum service temperature82deg CCured adhesive
Lap shear strength346psiAcid-etched aluminum-to-aluminum; 15 min cure at 25 deg C
Lap shear strength717psiAcid-etched aluminum-to-aluminum; 30 min cure at 25 deg C
Lap shear strength1,700psiAcid-etched aluminum-to-aluminum; 60 min cure at 25 deg C
T-peel strength2.7pliAcid-etched aluminum-to-aluminum; tested at 25 deg C