ROYAL DOUBLE BUBBLE 04007

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

ROYAL DOUBLE BUBBLE 04007

Main features

  • High-Peel Vibration-Resistant Bonding
  • Extended 3-Hour Working Window
  • 121 deg C Service Capability

Product Description

Hardman Double/Bubble 04007 Very High Peel Strength Epoxy is a 3.5 g premeasured, two-part structural epoxy packet with a semi-rigid cured profile and high peel performance. The gray mixed adhesive has a 50,000 cP viscosity at 25 deg C, a 3 hour work time, and an 18 hour handling time. After a 7 day cure at 25 deg C, typical T-peel strength reaches 24 pli and lap shear strength reaches 2,800 psi on acid-etched aluminum. The cured material has 65 Shore D hardness and a maximum service temperature of 121 deg C. It is used for repair and bonding where vibration, impact, shock, or peel loading is important.

Key features

  • High-peel semi-rigid cure: Typical T-peel strength is 24 pli on acid-etched aluminum after a 7 day cure at 25 deg C.
  • Extended 3-hour work time: The long open window supports placement and alignment before handling.
  • Elevated-temperature capability: The cured adhesive has a maximum service temperature of 121 deg C.

Applications

Applications include structural bonding and repair of industrial parts, sports equipment, marine and transportation parts, grinding-wheel hubs, and door or window gaskets where peel, vibration, impact, or shock resistance is required.

Product Family

ROYAL DOUBLE BUBBLE 04007

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Service temperature
121 °C

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Package size3.5gPremeasured dual-pouch packet
ColorGray-Mixed adhesive
Mixed viscosity50,000cPAt 25 deg C
Mixed specific gravity1.27-At 25 deg C
Work time3hAt room temperature
Handling strength18hAt room temperature
Shelf life24monthsPart A and Part B
Technical properties

After processing / final state

Property Value Unit Method / condition
Hardness65Shore DTested at 25 deg C
Maximum service temperature121deg CCured adhesive
Lap shear strength2,800psiAcid-etched aluminum-to-aluminum; 7 day cure at 25 deg C; tested at 25 deg C
T-peel strength24pliAcid-etched aluminum-to-aluminum; 7 day cure at 25 deg C; tested at 25 deg C
Lap shear strength3,206psiAcid-etched aluminum-to-aluminum; 7 day cure at 25 deg C; tested at -40 deg C
Lap shear strength970psiAcid-etched aluminum-to-aluminum; 7 day cure at 25 deg C; tested at 82 deg C

Leading Brands Trust in Our Products and Services