ROYAL DOUBLE BUBBLE 04006

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

ROYAL DOUBLE BUBBLE 04006

Main features

  • Low-Viscosity Thin-Bondline Flow
  • Extended 45-Minute Working Window
  • Progressive Room-Temperature Strength Build

Product Description

Hardman Double/Bubble 04006 Regular-Setting Epoxy combines a 3.5 g premeasured dual-pouch format with a low-viscosity, two-part epoxy for thin glue lines. The light-amber mixed adhesive has a viscosity of 3,700 cP at 25 deg C, a 45 minute work time, and a 4 hour handling time. It sets in a 10 mil film at room temperature and develops typical lap shear strength from 500 psi after 3 hours to 2,900 psi after two weeks on acid-etched aluminum. The cured material reaches 78 Shore D hardness and is used for furniture, hobby, and sports-equipment repair on supported aluminum, epoxy, phenolic, and wood surfaces.

Key features

  • Thin glue-line flow: The 3,700 cP mixed viscosity is suited to a 10 mil adhesive film.
  • 45-minute work time: The defined working window supports placement before the 4 hour handling stage.
  • Progressive room-temperature strength: Lap shear rises from 500 psi after 3 hours to 2,900 psi after two weeks on acid-etched aluminum.

Applications

Applications include thin glue-line bonding and repair for furniture, hobby projects, and sports equipment using supported aluminum, epoxy, phenolic, and wood surfaces.

Product Family

ROYAL DOUBLE BUBBLE 04006

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Service temperature
52 °C

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Package size3.5gPremeasured dual-pouch packet
ColorLight amber-Part A, Part B, and mixed adhesive
Mixed viscosity3,700cPAt 25 deg C
Work time45minAt room temperature
Tack-free time60minAt room temperature
Handling strength4hAt room temperature
Shelf life24monthsPart A and Part B
Technical properties

After processing / final state

Property Value Unit Method / condition
Hardness78Shore DTested at 25 deg C
Impact strength6.7ft-lbTested at 25 deg C
Maximum service temperature52deg CCured adhesive
Lap shear strength500psiAcid-etched aluminum-to-aluminum; 3 h cure at 25 deg C
Lap shear strength2,000psiAcid-etched aluminum-to-aluminum; 24 h cure at 25 deg C
Lap shear strength2,900psiAcid-etched aluminum-to-aluminum; 2 week cure at 25 deg C