ROYAL DOUBLE BUBBLE 04004

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

ROYAL DOUBLE BUBBLE 04004

Main features

  • Water-Clear Bondline Appearance
  • Self-Leveling Solventless Flow
  • Extended 60-Minute Working Window

Product Description

Hardman Double/Bubble 04004 Water-Clear Epoxy is a 3.5 g premeasured, two-part epoxy packet that cures to a transparent, water-clear bondline. The solventless liquid is self-leveling and blush-free, with a mixed viscosity of 14,000 cP at 25 deg C and a 60 minute work time. Handling strength develops in 8 hours, while the stated cured-property schedule uses 7 days at 25 deg C. Typical final properties include 85 Shore D hardness, 18 ft-lb impact strength, and up to 2,400 psi lap shear on acid-etched aluminum after one week. The clear system fits repairs and assemblies where bondline appearance matters.

Key features

  • Water-clear cured appearance: The transparent adhesive is used where the finished bondline remains visible.
  • Self-leveling solventless flow: The 14,000 cP mixed liquid levels across prepared surfaces without a solvent carrier.
  • Extended assembly window: A 60 minute work time and 8 hour handling point allow deliberate placement.

Applications

Applications include clear bonding and repair of glass, ceramics, metal, wood, selected plastics, printed circuit boards, optical components, jewelry, and art objects.

Product Family

ROYAL DOUBLE BUBBLE 04004

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Service temperature
82 °C

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Package size3.5gPremeasured dual-pouch packet
ColorClear-Part A, Part B, and mixed adhesive
Mix ratio1:1-Two-part system
Mixed viscosity14,000cPAt 25 deg C
Work time60minAt room temperature
Tack-free time180minAt room temperature
Handling strength8hAt room temperature
Shelf life24monthsPart A and Part B
Technical properties

After processing / final state

Property Value Unit Method / condition
Hardness85Shore D7 day cure at 25 deg C; tested at 25 deg C
Impact strength18ft-lbTested at 25 deg C
Maximum service temperature82deg CCured adhesive
Lap shear strength500psiAcid-etched aluminum-to-aluminum; 5 h cure at 25 deg C
Lap shear strength1,200psiAcid-etched aluminum-to-aluminum; 24 h cure at 25 deg C
Lap shear strength1,800psiAcid-etched aluminum-to-aluminum; 72 h cure at 25 deg C
Lap shear strength2,400psiAcid-etched aluminum-to-aluminum; 1 week cure at 25 deg C

Leading Brands Trust in Our Products and Services