RESIN DESIGNS EMI-CSI-M3

Harmonization Code : 3907.30.00.15 | Epoxide resin, halogen-free

RESIN DESIGNS EMI-CSI-M3

Main features

  • Combined EMI Shielding and Sealing
  • No-Mix Precured Rope Installation
  • -40 to 150 deg C Operation

Product Description

Resin Designs EMI-CSI-M3 Gel Rope Gasket is a configurable, precured silicone-gel-impregnated Monel wire-mesh rope for EMI shielding, electrical grounding, corrosion protection, environmental sealing, and pressure sealing. The construction uses knitted Monel mesh formed into a circular cross section and impregnated with silicone gel before supply. Because the gel is already cured, the gasket is installed as a preformed shielding and sealing element rather than mixed or cured in place. The family is available in multiple rope diameters and lengths and operates from -40 to 150 deg C. EMI-CSI-M3 is used where compatible assemblies require combined electrical grounding and environmental sealing.

Key features

  • Combined shielding and sealing: The Monel mesh and silicone gel construction provides EMI shielding, grounding, corrosion protection, and environmental sealing.
  • Precured rope construction: The silicone gel is cured before supply for installation as a preformed circular rope gasket.
  • Wide operating range: The gasket family operates from -40 to 150 deg C.

Applications / Suitable for

  • EMI shielding and electrical grounding.
  • Corrosion protection and environmental sealing.
  • Pressure sealing in compatible assemblies.
Product Family

RESIN DESIGNS EMI-CSI-M3

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Operating Temperature
-40 to 150 °C

Additional Information

Technical properties

As supplied / before processing

Rows describe the supplied rope construction and family format.

Property Value Unit Method / condition
Mesh materialMonel wire mesh-Knitted construction
Mesh formCircular rope-Circular cross section
Gel constructionPrecured silicone gel-Impregnated into the wire-mesh rope
Available configurationMultiple diameters and lengths-Configurable product family