PLEXUS MA920

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA920

Main features

  • Fast 4-6 Minute Working Window
  • Low-Odor Structural Bonding
  • Balanced Strength and Elongation

Product Description

Plexus MA920 Methacrylate Structural Adhesive is a two-part, 10:1 low-odor system for structural bonding of thermoplastics, metals, and composites. The adhesive provides a 4-6 minute working time and reaches handling strength in 16-17 minutes, supporting rapid assembly where positioning time is limited. Typical cured tensile strength is 16.4-20.1 MPa with 30-50% elongation, and the maximum gap-fill value is 9.5 mm. Part A and Part B viscosities are 80-120 and 35-80 x 1,000 cP, respectively. MA920 is used on composites, engineered thermoplastics, coated metals, and PC-120-conditioned raw metals.

Key features

  • Fast assembly window: A 4-6 minute working time and 16-17 minute handling time support rapid part positioning and assembly.
  • Low-odor technology: The two-part methacrylate system uses odor-blocking technology for lower-odor structural bonding.
  • Strength and elongation balance: Typical cured tensile strength of 16.4-20.1 MPa is paired with 30-50% elongation.

Applications / Suitable for

  • Structural bonding of thermoplastic, metal, and composite assemblies requiring a short working window.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two part (A / B)
Physical Properties
VOC
< 1
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
30 - 50 %

Additional Information

Technical properties

As supplied / before processing

Values apply to the matched 10:1 Part A and Part B system.

Property Value Unit Method / condition
Mix ratio by volume10:1-Part A adhesive to Part B activator
Part A viscosity80-120x 1,000 cPTypical as supplied
Part B viscosity35-80x 1,000 cPTypical as supplied
Working time4-6minMixed adhesive
Handling time16-17minTypical assembly handling time
Technical properties

After processing / final state

Values are typical and do not represent universal joint performance across all substrates.

Property Value Unit Method / condition
Tensile strength16.4-20.1MPaTypical cured material
Elongation30-50%Typical cured material
Maximum gap fill9.5mmMaximum stated joint gap