PLEXUS MA830

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA830

Main features

  • 4-6 Minute Working Time
  • Fast Primerless Metal Assembly
  • 2,610-3,190 psi Tensile Strength

Product Description

Plexus MA830 Methacrylate Structural Adhesive is a fast-working, two-part methacrylate structural adhesive for primerless bonding of metals and for joining selected thermoplastics and composites. The 10:1 system provides a 4-6 minute working time, supporting rapid assembly cycles where parts can be positioned promptly. Typical values at 23 deg C include 2,610-3,190 psi tensile strength, 10-20% elongation, and a maximum gap fill of 0.50 in (12.7 mm). The cured adhesive is also characterized by fatigue resistance, impact resistance, toughness, and resistance to salt spray and other environmental factors.

Key features

  • Rapid working time: A 4-6 minute working window supports fast structural assembly cycles.
  • Primerless metal bonding: The adhesive bonds many raw and coated metals without a separate primer.
  • Structural performance: Typical tensile strength is 2,610-3,190 psi with 10-20% elongation.

Applications / Suitable for

  • Primerless structural bonding of raw and coated metals, thermoplastics, and composites where a short working window is required.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two part (A / B)
Physical Properties
VOC
< 1
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
10 - 20 %

Additional Information

Technical properties

As supplied / before processing

Values are typical and are reported at 23 deg C unless otherwise noted.

Property Value Unit Method / condition
Mix ratio10:1-Two-part system
Working time4-6minTypical at 23 deg C
Part A viscosity80-120x 1,000 cPTypical at 23 deg C
Part B viscosity35-80x 1,000 cPTypical at 23 deg C
Maximum gap fill0.50 (12.7)in (mm)Typical joint-design value
Technical properties

After processing / final state

Values are typical; qualitative durability characteristics retain their product-level scope.

Property Value Unit Method / condition
Tensile strength2,610-3,190psiTypical cured material at 23 deg C
Elongation10-20%Typical cured material at 23 deg C
DurabilityFatigue, impact, and toughness resistance-Qualitative cured-joint characteristic
Environmental resistanceSalt spray and environmental factors-Qualitative cured-joint characteristic

Leading Brands Trust in Our Products and Services