PLEXUS MA8120

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA8120

Main features

  • Low-Halogen Primerless System
  • Broad Coated-Metal Adhesion
  • Salt-Spray Environmental Resistance

Product Description

Plexus MA8120 Methacrylate Structural Adhesive pairs a low-halogen, two-part methacrylate system with direct bonding of metal, plastic, and composite assemblies. The 1:1 formulation provides primerless adhesion to raw and coated metals, including hot-dip galvanized surfaces, as well as most thermoplastics and composites. Its lower-odor formulation combines high strength and elongation with fatigue resistance, impact resistance, and toughness. Environmental resistance includes salt-spray exposure and related environmental factors. MA8120 is suited to industrial and transportation structures that require broad substrate coverage without a separate metal-primer step.

Key features

  • Low-halogen formulation: The two-part adhesive is positioned for direct-to-metal structural assembly.
  • Primerless substrate range: It bonds raw and coated metals, thermoplastics, and composites without a separate metal primer.
  • Durable cured behavior: High strength and elongation are combined with fatigue, impact, and environmental resistance.

Applications / Suitable for

  • Industrial and transportation structural assemblies using raw or coated metals, thermoplastics, or composites.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two part (A / B)
Physical Properties
VOC
< 0.5
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
30 - 60 %

Additional Information

Technical properties

As supplied / before processing

Rows apply to the base MA8120 product; version-specific glass-bead values are not included.

Property Value Unit Method / condition
Component countTwo-part-Part A adhesive and Part B activator
Mix ratio1:1-Equal-ratio system
Halogen profileLow halogen-Product formulation
Odor profileLower odor-Product formulation
Technical properties

After processing / final state

Qualitative rows apply to the base MA8120 product and preserve the stated substrate scope.

Property Value Unit Method / condition
Primerless adhesionRaw and coated metals-Includes hot-dip galvanized surfaces; also supports thermoplastics and composites
Mechanical responseHigh strength and elongation-Qualitative cured-joint characteristic
DurabilityFatigue, impact, and toughness resistance-Qualitative cured-joint characteristic
Environmental resistanceSalt spray and environmental factors-Qualitative cured-joint characteristic