Plexus® MA8110 | Two-Part Methacrylate Adhesive

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Plexus® MA8110 | Two-Part Methacrylate Adhesive

Main features

  • 1:1 Controlled Mixing
  • 9 to 11-Minute Working Window
  • 24.8 MPa Cured Tensile Strength

Product Description

PLEXUS® MA8110 Methacrylate Adhesive is a two-part, 1:1 methacrylate structural adhesive for direct bonding to many metal substrates, including galvanized G60 and G90 steel, and for selected thermoplastic and composite assemblies. The gray, non-sag mixed adhesive provides a typical 9 to 11 minute working time at 23°C and supports gap-filling bondlines from 0.75 to 9.5 mm. It is documented for limited surface preparation on supported substrates and develops high tensile and lap-shear properties after cure.

Key features

  • Direct-to-metal bonding: The adhesive is documented for primerless bonding to many metals, including galvanized G60 and G90 steel.
  • 9 to 11-minute working time: The documented process window is measured at 23°C.
  • Gap-filling cured bond: The adhesive supports 0.75 to 9.5 mm bondlines with typical tensile strength of 21.4 to 24.8 MPa.

Applications / Suitable for

  • Structural bonding of galvanized and other metal assemblies
  • Selected thermoplastic bonding
  • Composite assembly bonding

Technical Specifications

General Properties
Color
The color
Off-White / Gray
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Adhesive / Activator)
Density (g)
0.97 / 0.96 g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1.01 / 1.0
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
11 °C
Operating Temperature
-40-82 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Color, Part A Off-white N/A As supplied
Color, Part B Gray N/A As supplied
Mix ratio 1:1 parts by volume Part A : Part B
Mix ratio 1:1 parts by weight Part A : Part B
Viscosity, Part A 40,000 to 70,000 cP As supplied
Viscosity, Part B 40,000 to 70,000 cP As supplied
Working time 9 to 11 min At 23°C
Shelf life 7 months Stored at 12 to 23°C
Technical properties

After-processing / final-state properties

Typical final-state values under the stated conditions. These values are not sales specifications.

Property Value Unit Method / condition
Recommended bondline gap 0.75 to 9.5 mm Documented range
Tensile strength 21.4 to 24.8 MPa ASTM D638
Tensile modulus 690 to 900 MPa Typical cured value
Tensile strain 10 to 20 % Typical cured value
Lap shear strength 12.4 to 15.8 MPa ASTM D1002
Operating temperature range -40 to 82 °C Documented range

Leading Brands Trust in Our Products and Services