PLEXUS MA8105

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA8105

Main features

  • Primerless Multi-Material Bonding
  • Easy 1:1 Mixing
  • Low-Odor Non-Filled Formulation

Product Description

Plexus MA8105 Methacrylate Structural Adhesive is a direct-to-metal, two-part methacrylate structural adhesive for industrial and transportation assemblies. The 1:1 system supports primerless bonding to raw and coated metals, including galvanized steel, and also bonds thermoplastics, polyamides such as nylon, and composites. Its low-odor, non-filled formulation is paired with high strength, high elongation, toughness, and fatigue resistance for dissimilar-material joints. MA8105 cures tack-free and is suited to multi-material assembly where reducing primer steps and using a simple equal-ratio mix can streamline the bonding process.

Key features

  • Primerless metal adhesion: The adhesive bonds raw, coated, and galvanized metals without a separate primer step.
  • Broad material coverage: Supported substrates include polyamides, other thermoplastics, and composites.
  • Equal-ratio processing: The 1:1 two-part system simplifies proportioning and cures to a tack-free surface.

Applications / Suitable for

  • Industrial and transportation assemblies using raw or coated metals, galvanized steel, polyamides, other thermoplastics, or composites.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two part (A / B)
Physical Properties
VOC
< 0.5
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
5 - 10 %

Additional Information

Technical properties

As supplied / before processing

MA8105 GB glass-bead values are excluded from this base-product table.

Property Value Unit Method / condition
Component countTwo-part-Part A adhesive and Part B activator
Mix ratio1:1-Equal-ratio system
FormulationNon-filled-Base MA8105 product
Odor profileLow odor-As supplied and during cure
Technical properties

After processing / final state

Qualitative rows apply to the base MA8105 product and preserve the stated substrate scope.

Property Value Unit Method / condition
Primerless adhesionRaw, coated, and galvanized metals-Also supports selected thermoplastics, nylon, and composites
Mechanical responseHigh strength and high elongation-Qualitative cured-joint characteristic
Fatigue behaviorHigh fatigue resistance-Qualitative cured-joint characteristic
Cured surfaceTack-free-After cure

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers