PLEXUS MA590

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA590

Main features

  • 90-105 Minute Working Time
  • Up to 38.1 mm Gap Fill
  • >130% Typical Elongation

Product Description

Plexus MA590 Methacrylate Structural Adhesive provides an extended-working-time 1:1 methacrylate system for structural bonding of large composite, thermoplastic, and metal assemblies. Its 90-105 minute working time supports prolonged positioning, while the highly thixotropic consistency maintains a gap-filling bead. Typical values include a maximum gap fill of 1.5 in (38.1 mm), tensile strength of 1,880-2,750 psi, and elongation above 130%. This combination is relevant to large structures where parts must be aligned over a longer period while retaining a non-sag adhesive bead and a high-toughness cured joint.

Key features

  • Long positioning window: A 90-105 minute working time supports extended assembly of large structures.
  • High-build gap filling: The thixotropic 1:1 system supports a maximum gap fill of 1.5 in (38.1 mm).
  • Highly extensible bondline: Typical elongation exceeds 130%, with tensile strength of 1,880-2,750 psi.

Applications / Suitable for

  • Large composite, thermoplastic, and metal assemblies that require a long working window.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two part (A / B)
Physical Properties
VOC
< 0.5
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
>130 %

Additional Information

Technical properties

As supplied / before processing

Values are typical and are reported at 23 deg C unless otherwise noted.

Property Value Unit Method / condition
Mix ratio1:1-Two-part system
Working time90-105minTypical at 23 deg C
Part A viscosity140-230x 1,000 cPTypical at 23 deg C
Part B viscosity165-230x 1,000 cPTypical at 23 deg C
Maximum gap fill1.5 (38.1)in (mm)Typical joint-design value
Technical properties

After processing / final state

Values are typical and do not represent universal joint performance across all substrates.

Property Value Unit Method / condition
Tensile strength1,880-2,750psiTypical cured material at 23 deg C
Elongation>130%Typical cured material at 23 deg C
ToughnessHigh-Qualitative cured-joint characteristic

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers