PLEXUS MA530

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA530

Main features

  • 30-40 Minute Working Time
  • Up to 18 mm Gap Tolerance
  • 90-160% Typical Elongation

Product Description

Plexus MA530 Methacrylate Structural Adhesive is a 1:1, non-sag methacrylate system for structural bonding of large composite, thermoplastic, and metal assemblies. The mixed adhesive forms a gray gel and provides a typical 30-40 minute working time at 23.9 deg C. Its 0.75-18.0 mm gap tolerance supports joints with wider dimensional variation, while the cured material combines 17.2-24.1 MPa tensile strength with 90-160% elongation. MA530 is suited to transportation, marine, and industrial structures that need a moderate open time, substantial gap filling, and a tough cured bondline for large-part assembly.

Key features

  • Moderate open time: A typical 30-40 minute working time at 23.9 deg C supports large-part assembly.
  • Substantial gap tolerance: The adhesive accommodates typical gaps from 0.75 to 18.0 mm.
  • High elongation: The cured material provides typical elongation of 90-160% with 17.2-24.1 MPa tensile strength.

Applications / Suitable for

  • Large composite, thermoplastic, and metal structures in transportation, marine, and industrial manufacturing.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two part (A / B)
Physical Properties
VOC
< 0.5
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
90 -160 %

Additional Information

Technical properties

As supplied / before processing

Part A, Part B, and mixed-system values are identified by row. Values are typical.

Property Value Unit Method / condition
Part A colorWhite-As supplied
Part B colorBlack or white-Activator option
Mix ratio by volume1:1-Part A to Part B
Part A viscosity130-180x 1,000 cPAs supplied
Part B viscosity160-215 / 80-140x 1,000 cPBlack / white activator
Working time30-40minMixed adhesive at 23.9 deg C
Shelf life6monthsContinuous storage at 13-25 deg C
Technical properties

After processing / final state

Values describe the cured material or bonded joint under the stated method and condition.

Property Value Unit Method / condition
Gap tolerance0.75-18.0mmTypical cured-joint range
Hardness70Shore DCured material
Tensile strength17.2-24.1MPaISO 527
Tensile modulus551-827MPaISO 527
Elongation at break90-160%ISO 527
Lap shear on aluminum14.4MPaTypical; aluminum with PC120 recommended