PLEXUS MA440

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA440

Main features

  • Self-Leveling Two-Part System
  • 15 MPa Typical Tensile Strength
  • 121 deg C Air Service Limit

Product Description

Plexus MA440 Methacrylate Adhesive uses a two-part, self-leveling methacrylate system for structural bonding of thermoplastic, metal, and composite assemblies. The uncured material has a reported density of 0.980 g/cm3. Typical cured values include 15.0 MPa tensile strength, 20% elongation, a 0.300 GPa elastic modulus, and 9.50 MPa cohesive lap-shear strength under the stated ASTM methods. A maximum air service temperature of 121 deg C is also reported. These characteristics position MA440 for structural joints where a flowable adhesive and a balance of strength and moderate elongation are needed.

Key features

  • Self-leveling application: The two-part adhesive flows to wet structural joint surfaces.
  • Cured mechanical balance: Typical cured properties include 15.0 MPa tensile strength and 20% elongation.
  • Elevated-temperature range: The reported maximum air service temperature is 121 deg C.

Applications / Suitable for

  • Structural bonding of thermoplastic, metal, and composite assemblies.
Product Family

PLEXUS MA440

Loading pricing…

Technical Specifications

General Properties
Density (g)
0.980 g/cm3
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
20 %

Additional Information

Technical properties

As supplied / before processing

Rows distinguish the uncured MA440 material and its two-part application form.

Property Value Unit Method / condition
Component countTwo-part-Part A adhesive and Part B activator
Application formSelf-leveling-Uncured adhesive
Density0.980g/cm3Uncured material
Technical properties

After processing / final state

Values describe the cured material under the stated ASTM method or service condition.

Property Value Unit Method / condition
Tensile strength15.0MPaASTM D638
Elongation at break20%ASTM D638
Elastic modulus0.300GPaASTM D638
Cohesive lap-shear strength9.50MPaASTM D1002
Maximum air service temperature121deg CCured material