PLEXUS MA425

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA425

Main features

  • 30-35 Minute Working Time
  • Non-Sag Thixotropic Dispensing
  • 30-50% Typical Elongation

Product Description

Plexus MA425 Methacrylate Structural Adhesive combines a two-part 10:1 methacrylate system with a 30-35 minute working window for structural bonding of composite, thermoplastic, and metal assemblies. Its non-sag thixotropic consistency supports controlled dispensing on structural joints and helps the bead remain in place during assembly. Typical cured tensile strength is 2,565-3,315 psi with 30-50% elongation, combining load-bearing capability with joint flexibility. The product is used in transportation and marine manufacturing for composite bonding and for joining thermoplastics, coated metals, and raw metals prepared with PC120 cleaner/conditioner.

Key features

  • Extended assembly time: A 30-35 minute working window supports structural bonding of larger or more complex assemblies.
  • Non-sag dispensing: Thixotropic flow helps the adhesive remain in place during application.
  • Strength with elongation: Typical tensile strength is 2,565-3,315 psi with 30-50% elongation.

Applications / Suitable for

  • Transportation and marine structural assemblies using composites, thermoplastics, coated metals, or PC120-prepared raw metals.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two part (A / B)
Physical Properties
VOC
<1
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
30 - 50 %

Additional Information

Technical properties

As supplied / before processing

Values are typical. Viscosity and gap data are reported at 23 deg C unless otherwise noted.

Property Value Unit Method / condition
Mix ratio10:1-Two-part system
Working time30-35minMixed adhesive
Part A viscosity100-125x 1,000 cPTypical at 23 deg C
Part B viscosity35-70x 1,000 cPTypical at 23 deg C
Maximum gap fill0.375 (9.5)in (mm)Typical joint-design value
Technical properties

After processing / final state

Values are typical and do not represent universal joint performance across all substrates.

Property Value Unit Method / condition
Tensile strength2,565-3,315psiTypical cured material at 23 deg C
Elongation30-50%Typical cured material at 23 deg C
Fatigue resistanceHigh-Qualitative cured-joint characteristic

Leading Brands Trust in Our Products and Services