PLEXUS MA330

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PLEXUS MA330

Main features

  • Extended 15-18 Minute Work Window
  • Defined 30-45 Minute Fixture
  • High-Strength 1:1 Structural Bonding

Product Description

Plexus MA330 uses a two-part, 1:1 methacrylate system for structural bonding of thermoplastics, metals, and composites. At 74 deg F (23 deg C), the non-sagging adhesive provides a 15-18 minute work time and a 30-45 minute fixture time, giving operators time for part alignment before fixture. It fills gaps from 0.75 to 3.2 mm and has an operating range of -55 to 121 deg C. Typical cured tensile strength is 24.1-31.0 MPa, with 20.7-24.1 MPa cohesive lap shear at a 0.76 mm gap.

Key features

  • 15-18 Minute Work Window: Provides extended time for positioning at 74 deg F (23 deg C).
  • 30-45 Minute Fixture: Develops handling strength within a defined room-temperature interval.
  • 24.1-31.0 MPa Tensile Strength: Forms a high-strength cured methacrylate bond.

Applications

Applications include structural bonding of supported ABS, acrylic, FRP, gelcoat, PVC, polyesters, steel, aluminum, stainless steel, styrenics, urethanes, and vinyl esters.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two part (Adhesive / Activator)
Physical Properties
VOC
<1
Other Properties
Storage Temperature
13 - 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical for the separate components and processing at 74 deg F (23 deg C) where stated.

Property Value Unit Method / condition
Component color - adhesive / activatorWhite / blackTypical uncured
Mix ratio by volume1:1Adhesive to activator
Component density - adhesive1.04g/ccTypical uncured
Component density - activator0.97g/ccTypical uncured
Component viscosity - adhesive / activator40,000-70,000 / 40,000-70,000cPTypical uncured at room temperature
Work time15-18minutesAt 74 deg F (23 deg C)
Fixture time30-45minutesAt 74 deg F (23 deg C)
Shelf life - adhesive / activator7 / 13monthsRecommended storage conditions
Technical properties

After-processing / final-state properties

Values are typical cured properties; lap-shear results apply only to the stated substrate and test method.

Property Value Unit Method / condition
Gap filling range0.75-3.2mmTypical joint range
Operating temperature-55 to 121deg CProduct operating range
Tensile strength24.1-31.0MPaASTM D638; cured at room temperature
Tensile modulus1,034-1,207MPaASTM D638; cured at room temperature
Strain to failure5-15%ASTM D638; cured at room temperature
Cohesive lap shear strength20.7-24.1MPaASTM D1002; 0.76 mm gap