PLEXUS MA320

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA320

Main features

  • Controlled 10-11 Minute Assembly
  • Broad 0.75-9.5 mm Gap Range
  • Flexible 40-80% Cured Elongation

Product Description

Plexus MA320 is a two-part, 10:1 methacrylate adhesive for structural bonding of thermoplastic, metal, and composite assemblies in transportation, marine, wind-energy, and engineering-construction applications. The non-sagging grade provides a 10-11 minute work time at 75 deg F (23.9 deg C) and a 0.75-9.5 mm gap tolerance. Typical cured properties include 12.4-15.2 MPa tensile strength, 40-80% elongation, and 64 Shore D hardness. The formulation is supplied in white, off-white, or black and provides toughness at low temperatures.

Key features

  • 10-11 Minute Work Window: Provides controlled assembly time at 75 deg F (23.9 deg C).
  • 0.75-9.5 mm Gap Tolerance: Supports varied structural joint thicknesses.
  • 40-80% Cured Elongation: Typical cured elongation is 40-80%.

Applications

Applications include structural bonding in transportation, marine, wind-energy, and engineering-construction assemblies using supported thermoplastics, metals, and composites.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two part (Adhesive / Activator)
Density (g)
0.93 g/cm3
Other Properties
Storage Temperature
13 - 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical for the separate components and processing at 75 deg F (23.9 deg C) where stated.

Property Value Unit Method / condition
Component color - Part A / Part BOff-white / whiteTypical uncured; other supplied colors are listed
Mix ratio by volume10:1Part A to Part B
Mix ratio by weight6.18:1.00Part A to Part B
Component density - Part A0.92g/mLTypical uncured
Component density - Part B1.51g/mLTypical uncured
Component viscosity - Part A / Part B135-175 / 35-70x 1,000 cPTypical uncured
Work time10-11minutesAt 75 deg F (23.9 deg C)
Time to 500 psi (3.4 MPa)38-40minutesAt 75 deg F (23.9 deg C)
Technical properties

After-processing / final-state properties

Values are typical cured properties; lap-shear results apply only to the stated substrate and test method.

Property Value Unit Method / condition
Gap tolerance0.75-9.5mmTypical cured joint range
Hardness64Shore DTypical cured property
Tensile strength12.4-15.2MPaASTM D638 / ISO 527
Tensile modulus469-634MPaASTM D638 / ISO 527
Elongation at break40-80%ASTM D638 / ISO 527
Lap shear - aluminum14.9MPaASTM D1002; cohesive failure
Lap shear - stainless steel18.6MPaASTM D1002; cohesive failure
Lap shear - GRP14.4MPaASTM D1002; fiber tear