PLEXUS MA300/3000

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA300/3000

Main features

  • Simple 1:1 Meter-Mix Processing
  • Fast 3-6 Minute Assembly
  • High-Strength Stiff Cured Bond

Product Description

Plexus MA300 pairs a two-part, 1:1 methacrylate system with structural bonding of thermoplastics, metals, and composites. At 74 deg F (23 deg C), the non-sagging adhesive provides a 3-6 minute work time, reaches 500 psi (3.4 MPa) in 11-13 minutes, and reaches 1,000 psi (6.9 MPa) in 13-16 minutes. Typical cured tensile strength is 24.2-29.6 MPa with 20-40% elongation and 78 Shore D hardness. Applications include supported ABS, acrylic, FRP, gelcoat, PVC, steel, aluminum, polyester, styrenic, urethane, and vinyl-ester assemblies.

Key features

  • Simple 1:1 Mixing: Uses equal component volumes for cartridge or meter-mix dispensing.
  • 3-6 Minute Work Window: Supports rapid assembly at 74 deg F (23 deg C).
  • 24.2-29.6 MPa Tensile Strength: Provides a high-strength cured methacrylate bond.

Applications

Applications include structural bonding of supported thermoplastics, metals, and composites, including ABS, acrylic, FRP, gelcoat, PVC, steel, aluminum, polyesters, styrenics, urethanes, and vinyl esters.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two part (A | B)
Physical Properties
VOC
< 1 %
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
20 - 40 %

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical for the separate components and processing at 75 deg F (23.9 deg C) where stated.

Property Value Unit Method / condition
Component color - Part A / Part BBeige / off-whiteTypical uncured
Mix ratio by volume1:1Part A to Part B
Component density - Part A1.00g/mLTypical uncured; +/- 0.02
Component density - Part B0.96g/mLTypical uncured; +/- 0.02
Component viscosity - Part A / Part B40-70 / 40-70x 1,000 cPTypical uncured
Work time3-6minutesAt 75 deg F (23.9 deg C)
Time to 500 psi (3.4 MPa)11-13minutesAt 75 deg F (23.9 deg C)
Shelf life13monthsRecommended storage conditions
Technical properties

After-processing / final-state properties

Values are typical cured properties; lap-shear results apply only to the stated substrate and test method.

Property Value Unit Method / condition
Gap tolerance0.25-3.2mmTypical cured joint range
Hardness78Shore DTypical cured property
Tensile strength24.2-29.6MPaASTM D638 / ISO 527
Tensile modulus1,524-2,062MPaASTM D638 / ISO 527
Elongation at break20-40%ASTM D638 / ISO 527
Lap shear - aluminum21.8MPaASTM D1002; adhesive failure
Lap shear - stainless steel23.1MPaASTM D1002; cohesive failure