PLEXUS MA2045

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA2045

Main features

  • Extended 45-50 Minute Work Window
  • Vertical Non-Sag Placement
  • Deep 38 mm Gap Bonding

Product Description

Plexus MA2045 is a two-part, 10:1 methacrylate adhesive for structural bonding of composite, thermoplastic, and metal assemblies where thick joints or vertical placement are required. The non-sagging formulation has a 45-50 minute work time at 75 deg F (23.9 deg C) and a typical gap tolerance of 0.75-38 mm. It is formulated to limit sag and slide on vertical surfaces and to avoid boiling in gaps up to 38 mm. Typical cured properties include 15.2-20.0 MPa tensile strength and 90-125% elongation.

Key features

  • 0.75-38 mm Thick-Gap Bonding: Accommodates unusually deep structural joints.
  • 45-50 Minute Work Window: Provides extended positioning time at 75 deg F (23.9 deg C).
  • Vertical Non-Sag Application: Limits sag and slide during placement on vertical surfaces.

Applications

Applications include structural bonding of composites, thermoplastics, and metals, including vertical-surface and thick-gap assemblies.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two part (A | B)
Physical Properties
VOC
< 1 %
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
90 - 125 %

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical for the separate components and processing at 75 deg F (23.9 deg C) where stated.

Property Value Unit Method / condition
Component color - Part A / Part BOff-white / blue or blackTypical uncured
Mix ratio by volume10:1Part A to Part B
Component density - Part A0.94g/mLTypical uncured
Component density - Part B1.07g/mLTypical uncured
Component viscosity - Part A180-220x 1,000 cPTypical uncured
Component viscosity - Part B35-70x 1,000 cPTypical uncured
Work time45-50minutesAt 75 deg F (23.9 deg C)
Time to 500 psi (3.4 MPa)100-105minutesAt 75 deg F (23.9 deg C)
Technical properties

After-processing / final-state properties

Values are typical cured properties; lap-shear results apply only to the stated substrate and test method.

Property Value Unit Method / condition
Gap tolerance0.75-38mmTypical cured joint range
Hardness74Shore DTypical cured property
Tensile strength15.2-20.0MPaISO 527
Tensile modulus413-689MPaISO 527
Elongation at break90-125%ISO 527
Lap shear - aluminum16.0MPaASTM D1002; cohesive failure

Leading Brands Trust in Our Products and Services