PLEXUS MA1020

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA1020

Main features

  • Very Low Cure Shrinkage
  • Fast 15-20 Minute Strength Build
  • Broad 0.75-9.5 mm Gap Range

Product Description

Plexus MA1020 is a two-part, 10:1 methacrylate adhesive with very low cure shrinkage and very low odor for structural bonding of thermoplastic, metal, and composite assemblies. At 74 deg F (23 deg C), it provides a 5-6 minute work time and reaches approximately 75% of ultimate strength in 15-20 minutes. The non-sagging blue system fills gaps from 0.75 to 9.5 mm. Typical cured properties include 9.0-11.0 MPa tensile strength, 10-20% elongation, and 65 Shore D hardness.

Key features

  • Very Low Cure Shrinkage: Provides a very low-shrinkage cure profile.
  • 5-6 Minute Working Time: Provides a defined assembly window at 74 deg F (23 deg C).
  • 15-20 Minute Strength Build: Reaches approximately 75% of ultimate strength at 74 deg F (23 deg C).

Applications

Applications include structural bonding of thermoplastics, metals, and composites, including plastic and composite assemblies where low odor and low cure shrinkage are important.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two part (A | B)
Physical Properties
VOC
< 1 %
Other Properties
Storage Temperature
13 - 25 °C
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
10 - 20 %

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical for the separate components and processing at 75 deg F (23.9 deg C) where stated.

Property Value Unit Method / condition
Component color - Part A / Part BOff-white / blue or blackTypical uncured
Mix ratio by volume10:1Part A to Part B
Component density - Part A0.93g/mLTypical uncured
Component density - Part B1.07g/mLTypical uncured
Component viscosity - Part A100-130x 1,000 cPTypical uncured
Component viscosity - Part B35-80x 1,000 cPTypical uncured
Work time5-6minutesAt 75 deg F (23.9 deg C)
Time to 500 psi (3.4 MPa)10-12minutesAt 75 deg F (23.9 deg C)
Technical properties

After-processing / final-state properties

Values are typical cured properties; lap-shear results apply only to the stated substrate and test method.

Property Value Unit Method / condition
Gap tolerance0.75-9.5mmTypical cured joint range
Hardness65Shore DTypical cured property
Tensile strength9.0-11.0MPaASTM D638 / ISO 527
Tensile modulus645-872MPaASTM D638 / ISO 527
Elongation at break10-20%ASTM D638 / ISO 527
Lap shear - aluminum13.2MPaASTM D1002; cohesive failure
Lap shear - carbon fiber10.2MPaASTM D1002; substrate failure

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers