PLEXUS H4110

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

PLEXUS H4110

Main features

  • Extended 8-12 Minute Work Window
  • Non-Sag Gel Placement
  • Elastic Mixed-Material Bonding

Product Description

Plexus H4110 is a two-part, 1:1 hybrid adhesive supplied as a non-sagging gel for elastic semi-structural bonding. It provides an 8-12 minute work time at 25 deg C for positioning composites, thermoplastics, metals, wood, concrete, and cement. The low-odor, low-exotherm formulation supports controlled application where a more elastic bond is preferred over a rigid structural joint. Its gel consistency limits slump during placement and keeps the mixed adhesive within the intended bond area across supported mixed-material assemblies.

Key features

  • 8-12 Minute Work Window: Allows measured part positioning at 25 deg C.
  • Non-Sag Gel Control: Maintains controlled placement during assembly.
  • Elastic Semi-Structural Bond: Forms an elastic bond for supported mixed-material assemblies.

Applications

Applications include bonding composites, thermoplastics, metals, wood, concrete, and cement.

Technical Specifications

Physical Properties
VOC
0 %
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
150 %
General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two part
Other Properties
Storage Temperature
10 - 24 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
System formTwo-part non-sagging gelAs supplied and mixed for application
Mix ratio by volume1:1Adhesive to activator
Work time8-12minutesAt 25 deg C
Exotherm characteristicLowMixed adhesive
Odor characteristicLowMixed adhesive