PLEXUS AO420

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS AO420

Main features

  • Controlled 4-6 Minute Assembly
  • Broad 0.75-9.5 mm Gap Range
  • Balanced Strength and Elongation

Product Description

Plexus AO420 / MA420 is a two-part, 10:1 methacrylate adhesive for structural bonding of thermoplastic, metal, and composite assemblies. At 75 deg F (23.9 deg C), the non-sagging system has a 4-6 minute work time and reaches 1,000 psi (6.9 MPa) in 20-22 minutes. Its 0.75-9.5 mm gap tolerance accommodates varied joint geometries, while typical cured properties include 16.8-20.5 MPa tensile strength, 20-40% elongation, and 73 Shore D hardness. Applications include composite bonding in transportation and other supported mixed-material assemblies.

Key features

  • 4-6 Minute Work Window: Provides controlled assembly time at 75 deg F (23.9 deg C).
  • 0.75-9.5 mm Gap Tolerance: Accommodates a broad range of structural joint thicknesses.
  • Balanced Strength and Elongation: Typical cured values combine 16.8-20.5 MPa tensile strength with 20-40% elongation.

Applications

Applications include structural bonding of thermoplastics, metals, and composites, including transportation composite assemblies.

Technical Specifications

General Properties
Chemistry Type
Methacrylate
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
2 Part (A | B)
Density (g)
0.97 | 1.05 g/cm3
Curing Conditions
Fixture Time
18– 22 minutes
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
11 °C
Operating Temperature
-55 to 121 °C

Additional Information

Structural adhesives

Plexus MA420 (AO420) Two-Part Methacrylate Structural Adhesive

Plexus MA420 is a two-part methacrylate structural adhesive system consisting of MA420 Part A adhesive and AO420 Part B activator. The components are mixed and used together as one adhesive system for bonding thermoplastics, metals, and composites. The system uses a 10:1 mix ratio by volume and provides a typical work time of 4-6 minutes at 75°F (23.9°C).

Two-part MMA adhesive system MA420 Part A + AO420 Part B 10:1 mix ratio by volume 4-6 min typical work time
Technical properties

MA420 / AO420 system properties

Part A and Part B properties are identified separately where they describe the materials before mixing. Mix ratios, work time, joint characteristics, and cured mechanical properties apply to the combined MA420 / AO420 adhesive system.

Mix ratio by volume
10:1
MA420 Part A to AO420 Part B.
Work time
4-6 min
Typical at 75°F (23.9°C).
Gap tolerance
0.75-9.5 mm
Typical cured joint range.

As-supplied and before-processing properties

Values are typical for the separate components and processing at 75°F (23.9°C) where stated.

Property Part A: MA420 Part B: AO420 Unit Method / condition
Color Off-white Off-white, blue, or black   Typical as supplied
Density 0.97 1.05 g/mL Typical as supplied
Viscosity 100-125 35-80 x 1,000 cP Typical as supplied
Mix ratio by volume 10 1 ratio Part A to Part B
Mix ratio by weight 9 1 ratio Part A to Part B
Work time 4-6 minutes Mixed system at 75°F (23.9°C)
Fixture time 18-22 minutes Mixed system at 23°C
Shelf life 10; 7 for black variant months Continuous storage at recommended conditions

Mixed-system and final cured properties

These values apply to the combined MA420 / AO420 system. Mechanical results remain specific to the stated test methods and substrates.

Property Value Unit Method / condition
Gap tolerance 0.75-9.5 mm Typical cured joint range
Hardness 73 Shore D Typical cured property
Tensile strength 16.8-20.5 MPa ASTM D638 / ISO 527
Tensile modulus 1,026-1,388 MPa ASTM D638 / ISO 527
Elongation at break 20-40 % ASTM D638 / ISO 527
Lap shear - aluminum 26.6 MPa ASTM D1002; adhesive failure
Lap shear - carbon fibre 23.1 MPa ASTM D1002; cohesive failure

Values are typical and are not specifications. Component-specific properties apply only before mixing, while joint and mechanical properties apply to the correctly mixed MA420 / AO420 system.

Processing

Preparing and applying the MA420 / AO420 adhesive system

MA420 Part A and AO420 Part B are prepared, mixed, dispensed, and assembled as one adhesive system. Maintain the specified mix ratio and complete assembly within the available work-time window.

Stage 1
Condition and clean
Apply the adhesive at 18-30°C (65-85°F). Bonding surfaces should be clean, dry, and free of grease, dirt, and other contamination.
Stage 2
Prepare substrates
Prepare thermoplastic, metal, or composite surfaces as required for the specific substrate condition. Composite surfaces should remain free of dust and mold-release contamination.
Stage 3
Mix and dispense
Combine MA420 Part A and AO420 Part B at 10:1 by volume or 9:1 by weight. When using a static mixer, purge the mixer before dispensing material for the bonded assembly.
Stage 4
Assemble and fixture
Mate the parts within the 4-6 minute typical work-time window at 23.9°C and maintain fixture support until sufficient handling strength develops.
Storage and handling

Maintain both components under controlled storage conditions

Store MA420 Part A and AO420 Part B continuously at 13-25°C. Temperatures above 27°C reduce shelf life, and storage above 38°C should be avoided. Storage at 7-18°C can extend product life; allow the material to return to room temperature before use. Typical shelf life is 10 months, or 7 months for the black variant, when maintained under the recommended storage conditions.

Next steps

Discuss Plexus MA420 with Krayden

Discuss the complete MA420 / AO420 two-part adhesive system, dispensing configuration, substrate preparation, joint geometry, work-time requirements, fixture planning, and package needs with Krayden. Share your substrates and assembly process so the technical team can help evaluate the complete adhesive system for your application.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers