PERMATEX 2BR

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

PERMATEX 2BR

Main features

  • Slow-Drying Gasket Dressing
  • Controlled Tacky Assembly
  • Fluid- and Heat-Resistant Sealing

Product Description

Permatex Form-A-Gasket No. 2 Sealant, 3 OZ is a black, viscous, slow-drying gasket-sealant paste supplied in a 3 oz tube for dressing cut gaskets and sealing flanges, threaded connections, hose connections, cover plates, and other semipermanent assemblies. The black, viscous material is applied as a thin, even film and air-dried until tacky before the parts are assembled. Typical operational time is 4 hours, with full cure after 24 hours. The continuous temperature range is -54 to 204 deg C, and the sealant retains effective properties with water, ethylene glycol, gasoline, motor oil, transmission fluid, and sea water.

Key features

  • Slow-Drying Gasket Dressing: The formulation supports gasket dressing and semipermanent reassembly.
  • Controlled Tacky Assembly: A thin film is air-dried until tacky before parts are tightened into position.
  • Fluid and Temperature Resistance: The sealant is rated for -54 to 204 deg C and the listed service fluids.

Applications

Applications include valve-cover and oil-pan gaskets, flanges, threaded and hose connections, cover plates, and semipermanent reassembly work.

Product Family

PERMATEX 2BR

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black paste
Chemistry Type
Modified resin, fillers & alcohol
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.5
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
Viscous paste mPa.s
Other Properties
Storage Temperature
8 - 28 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Chemical typeModified resin, fillers, and alcoholAs supplied
AppearanceBlack pasteAs supplied
OdorAlcoholicAs supplied
Specific gravity1.5Typical value
ViscosityViscous pasteAs supplied
Package size3ozTube; US item 80016
Technical properties

After-processing / final-state properties

Operational and cure times vary with temperature, humidity, and gap.

Property Value Unit Method / condition
Assembly operational time4hoursTypical after application
Full cure time24hoursTypical after application
Continuous temperature resistance-54 to 204deg CTypical range
Chemical and solvent resistanceWater, ethylene glycol, gasoline, motor oil, transmission fluid, sea waterRetains effective properties in contact