PERMABOND UV640

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND UV640

Main features

  • Fast Low-Power UV Cure
  • High-Elongation Plastic Bonding
  • Clear Polycarbonate Assembly

Product Description

Permabond UV640 is a single-part, medium-viscosity methacrylate adhesive developed for rapid UV bonding of plastics, including polycarbonate and acrylic. The clear liquid cures on demand across 365 to 420 nm, with typical fixture times from 2 to 10 seconds under the listed lamp conditions. At 25 deg C, viscosity is 3,000 to 5,000 mPa s at 20 rpm. The cured adhesive combines 13 N/mm^2 tensile strength with 110% elongation and 55 to 75 Shore D hardness, supporting plastic assemblies and joints between substrates with different coefficients of thermal expansion.

Key features

  • Fast Low-Power UV Cure: Typical fixture time is 2 to 10 seconds under the listed UV lamp conditions.
  • Medium-Viscosity Placement: Viscosity is 3,000 to 5,000 mPa s at 25 deg C and 20 rpm.
  • High-Elongation Cured Bond: The cured adhesive reaches 110% elongation with 13 N/mm^2 tensile strength.

Applications

Applications include bonding polycarbonate, acrylic, and other supported plastics, including assemblies with different coefficients of thermal expansion.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Colorless, clear
Refractive index
The refractive index determines how much the path of light is bent, or refracted, when entering a material. It is calculated by taking into account the velocity of light in vacuum compared to the velocity of light in the material. The refractive index calculation can be affected by the wavelength of light and the temperature of the material. Even though it is usually reported on standard wavelengths it is advised to check the TDS for the precise test parameters.
>1.490
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
3,000-5,000 | 12,000-25,000 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
110 %
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
25-30 kV/mm
Chemical Properties
Water Absorption
<5 %
Other Properties
Storage Temperature
5 - 25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Fixture time depends on lamp output, distance, and substrate transmission.

Property Value Unit Method / condition
Chemical compositionMethacrylate esterAs supplied
AppearanceColorless, clearAs supplied
Viscosity3,000 to 5,000mPa sAt 25 deg C; 20 rpm
Viscosity12,000 to 25,000mPa sAt 25 deg C; 2.5 rpm
Specific gravity1.1As supplied
Typical fixture time2 to 10secondsListed UV lamp conditions
Cure wavelength365 to 420nmMatch lamp output to the photoinitiator
Technical properties

After-processing / final-state properties

Values are typical cured properties for the stated methods and substrates.

Property Value Unit Method / condition
Overlap shear strength - polycarbonate>9N/mm^2ISO 4587; substrate failure observed
Overlap shear strength - acrylic>1.5N/mm^2ISO 4587; substrate failure observed
Tensile strength13N/mm^2ISO 37
Elongation at break110%ISO 37
Hardness55 to 75Shore DISO 868
Dielectric strength25 to 30kV/mmTypical cured value
Dielectric constant41 MHz at 25 deg C
Water absorption<5%ISO 62; 2 hours in boiling water