PERMABOND TA4610

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND TA4610

Main features

  • Underwater Structural Bonding
  • Primer-Free Polyolefin Assembly
  • Microparticle-Controlled 1 mm Gaps

Product Description

Permabond TA4610 is a two-part, 1:1 toughened acrylic adhesive for polypropylene, polyethylene, metals, composites, and dissimilar-material assemblies. It bonds low-surface-energy plastics without primer or surface treatment and supports water-resistant and underwater bonding. The thixotropic system contains microparticles for a maximum 1 mm gap. At 23 deg C, typical pot life is 5 to 8 minutes, fixture strength develops in 12 to 15 minutes, and handling strength in 40 to 50 minutes. Working strength develops in 6 to 8 hours, with cured shear strengths of 15 N/mm^2 on HDPE and 13 N/mm^2 on epoxy FRP.

Key features

  • Underwater Bonding Capability: Supports underwater bonding and water-resistant assemblies.
  • Primer-Free PP and PE: Bonds polypropylene and polyethylene without primer or surface treatment.
  • Microparticle Gap Control: Microparticles provide 1 mm maximum gap control for assembled joints.

Applications

Applications include underwater or water-resistant bonding, polypropylene and polyethylene assembly, and bonding metals, composites, and dissimilar substrates.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Off-white / Almost colorless
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
TA4610 A / TA4610 B
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
5-8 minutes
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.0 / 1.0
Other Properties
Maximum gap fill
1 mm
Storage Temperature
2 - 7 | 5 - 25 °C
Curing Conditions
Fixture Time
12-15 minutes

Additional Information

Technical properties

As-supplied / before-processing properties

Values identify the separate Part A and Part B components or the mixed adhesive, as stated.

Property Value Unit Method / condition
Part A viscosity200,000 to 500,000mPa sAt 25 deg C; thixotropic
Part B viscosity20,000 to 30,000mPa sAt 25 deg C
Specific gravity1.0Part A and Part B
Mix ratio1:1Part A to Part B
Maximum gap fill1mmContains microparticles for gap control
Pot life5 to 8minutes2 g + 2 g at 23 deg C
Fixture time12 to 15minutes0.1 N/mm^2 shear strength at 23 deg C
Handling time40 to 50minutes0.3 N/mm^2 shear strength at 23 deg C
Technical properties

After-processing / final-state properties

Strength values are typical cured results for the listed substrate combinations.

Property Value Unit Method / condition
Shear strength - polypropylene8N/mm^2Typical; substrate failure observed
Shear strength - polyethylene7N/mm^2Typical; substrate failure observed
Shear strength - HDPE15N/mm^2Typical
Shear strength - mild steel to PP7N/mm^2Typical
Shear strength - stainless steel to PP5N/mm^2Typical
Shear strength - aluminum to PP4N/mm^2Typical
Shear strength - carbon fiber8N/mm^2Typical
Shear strength - epoxy FRP13N/mm^2Typical

Leading Brands Trust in Our Products and Services