PERMABOND TA4592

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND TA4592

Main features

  • External-Mix Automated Dispensing
  • Sub-30-Second Gel Time
  • Motor Magnet and Ferrite Bonding

Product Description

Permabond TA4592 is a two-component, 1:1 external-mix structural acrylic adhesive for bonding magnets and ferrites in electric motors. Part A and Part B are dispensed separately and mixed as the beads fall onto the part, supporting high-speed automated assembly without a static mixer. The system fills gaps up to 1 mm, gels in less than 30 seconds, fixtures zinc in 10-30 seconds, and cures fully in 24 hours. Typical cured performance includes 20-25 N/mm2 shear strength on mild steel, 15-20 N/mm2 on zinc, and 10-20 kJ/m2 impact strength.

Key features

  • External-Mix Automation: Two dispensed components mix in air without a static mixer.
  • Sub-30-Second Gel: A 1 g plus 1 g mix gels in less than 30 seconds.
  • Motor Magnet and Ferrite Bonding: Targets magnet and ferrite attachment in electric-motor assembly.

Applications

Applications include automated bonding of magnets and ferrites in electric motors and supported structural acrylic assemblies.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Blue / Yellow-green
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
TA4592 A / TA4592 B
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1
Other Properties
Maximum gap fill
1 mm
Storage Temperature
2 - 7 °C
Curing Conditions
Fixture Time
10-30 seconds
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.1 W/m.K

Additional Information

Technical properties

As supplied / before processing

Part A and Part B are shown separately; processing values apply to the stated 1:1 external-mix system.

Property Value Unit Method / condition
AppearancePart A: blue; Part B: yellow-greenAs supplied
Part A viscosity10,000-15,000; 40,000-60,000mPa s20 rpm; 2.5 rpm at 25 deg C
Part B viscosity5,000-6,000; 12,000-15,000mPa s20 rpm; 2.5 rpm at 25 deg C
DensityPart A: 1.1; Part B: 1.1As supplied
Mix ratio1:1External mix
Maximum gap fill1mmTypical curing property
Cure milestonesGel: <30 seconds; zinc fixture: 10-30 seconds; full cure: 24 hoursGel based on 1 g Part A plus 1 g Part B
Storage temperature2 to 7deg CRecommended storage range
Technical properties

After processing / final state

Values are typical for cured adhesive and the stated substrates, cure periods, and methods.

Property Value Unit Method / condition
Shear strength - mild steel20-25N/mm2Typical cured value
Shear strength - zinc15-20N/mm2Typical cured value
Shear strength - steel to ferrite, 3 minutes4N/mm2Typical cure development
Shear strength - steel to ferrite, 24 hours>14N/mm2Substrate failure
Tensile strength25N/mm2ASTM D2095
Impact strength10-20kJ/m2ASTM D-950
Coefficient of thermal expansion80 x 10^-61/KASTM D-696
Thermal conductivity0.1W/(m K)ASTM C-177