PERMABOND LM012

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

PERMABOND LM012

Main features

  • Unfilled PFAS-Free Anaerobic Threadsealant
  • Sensitive High-Pressure Hydraulic-System Sealing
  • MIL-S-22473/ASTM D5363 Compliance Scope

Product Description

Permabond® LM012 is a PFAS-free, unfilled, medium-viscosity anaerobic threadsealant specially engineered for use in very sensitive, high-pressure hydraulic systems. Because it is formulated without fillers, any adhesive that accidentally squeezes out of the joint and into the hydraulic system safely disperses into the fluid without clogging or fouling fine hydraulic screens and valves. It cures at room temperature in the absence of air, forming a robust seal up to the burst rating of the pipe itself.

Key features

  • Hydraulic fluid compatible: Unfilled resin disperses into hydraulic fluids without leaving particles that could clog sensitive screens or valves.
  • Military and ASTM approved: Tested and certified to meet the lot requirements of MIL-S-22473 Grade HVV and ASTM D5363 AN 0163 Group 01 Class 6 Grade 3.
  • Safe and reliable: 100% solvent-free and PFAS-free formulation that delivers excellent chemical and temperature resistance while offering directional freedom during assembly.

Applications / Suitable for

  • Sealing threaded metallic pipe joints in sensitive, high-pressure hydraulic systems
  • Assemblies requiring compliance with MIL-S-22473 Grade HVV
  • Hydraulic component assembly where screen or valve fouling is a critical concern
Product Family

PERMABOND LM012

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Brown
Chemistry Type
Methacrylate esters
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
2,000 mPa.s
Other Properties
Maximum gap fill
0.2 mm
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.19 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Methacrylate esters - -
Appearance Brown - Liquid
Viscosity 2,000 mPa.s (cP) at 25°C
Specific Gravity 1.07 - 1.1 - -
Particle Size < 10 µm -
UV Fluorescence Yes - -
Flash Point > 93 °C (199.94°F)
Volatile Organic Compound < 2 % 20 grams/liter (Estimated)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Maximum Gap Fill 0.2 mm (0.008 in)
Maximum Thread Size M20 - (3/4")
Handling Strength Time 30 minutes M10 steel at 23°C
Full Strength Time 24 hours M10 steel at 23°C
Breakaway Torque Strength 3 N-m M10 steel (ISO 10964) (25 in.lb)
Prevailing Torque Strength 2 N-m M10 steel (ISO 10964) (15 in.lb)
Shear Strength 5 MPa Steel collar & pin (ISO 10123) (750 psi)
Coefficient of Thermal Expansion 90E-6 mm/m/°K -
Thermal Conductivity 0.19 W/(m.K) -