PERMABOND ASC10

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

PERMABOND ASC10

Main features

  • Anaerobic Cure on Passive Surfaces
  • Fast-Evaporating Non-Halogenated Surface Conditioner
  • Up to 30-Day Surface Activation

Product Description

Permabond® ASC10 Anaerobic Surface Conditioner is a rapid-drying accelerator formulated exclusively for use with anaerobic adhesives and sealants. It enables and accelerates the curing process on inactive or passive surfaces such as zinc plating, cadmium plating, stainless steel, gold, glass, and painted surfaces. Formulated with a non-halogenated, ozone-safe solvent, it simultaneously cleans contaminants from parts while leaving a thin deposit of initiator that remains active for up to 30 days before bonding.

Key features

  • Enables cure on passive surfaces: Triggers and accelerates the cure of anaerobic adhesives on difficult, inactive substrates.
  • Rapid drying and extended active life: Evaporates quickly while allowing treated parts to remain active for up to 30 days prior to assembly.
  • Environmentally conscious formula: Contains no ozone-depleting agents and utilizes a non-halogenated solvent.

Applications / Suitable for

  • Accelerating cure on inactive surfaces like stainless steel, zinc, cadmium, and glass
  • Improving cure speed in low-temperature environments
  • Enhancing the cure profile on poorly mated parts or wider gaps

Technical Specifications

General Properties
Color
The color
Blue Green
Evaporation Rate
4.3
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.73
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
-7 °C
Other Properties
Storage Temperature
5 to 25°C °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Appearance Blue Green - Liquid
Specific Gravity 0.73 - -
Flash Point -7 °C (-20°F)
Evaporation Rate 4.3 - (Butyl acetate = 1)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Active Life on Part 30 days After evaporation