PERMABOND 105

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND 105

Main features

  • 5 to 20-Second Fixture Time
  • Low-Viscosity Single-Component Adhesive
  • Hard-to-Bond Plastic and Rubber Bonding

Product Description

PERMABOND® 105 Cyanoacrylate Adhesive is a single-component, low-viscosity, high-purity ethyl cyanoacrylate adhesive developed for rapid bonding of hard-to-bond plastics and rubbers. Surface moisture initiates polymerization when the adhesive is pressed into a thin film between closely fitted parts. The colorless, 100% reactive formulation requires no mixing or heat cure and provides fixture or handling times of 5–20 seconds on documented substrates. Supported materials include natural rubber, Buna N rubber, EPDM, butyl rubber, ABS, PVC, polycarbonate, phenolic materials, and metals.

Key features

  • Rapid fixture performance: Typical fixture or handling times range from 5–20 seconds on documented rubber, plastic, phenolic, and steel substrates.
  • Low-viscosity application: A typical viscosity of 30–50 mPa·s at 25°C supports application into closely fitted joints with a maximum documented gap fill of 0.1 mm.
  • Single-component formulation: The 100% reactive ethyl cyanoacrylate system requires no mixing, solvent evaporation, or heat cure.

Applications / Suitable for

  • Bonding natural and synthetic rubbers, including Buna N, EPDM, and butyl rubber
  • Bonding hard-to-bond plastic components
  • Bonding ABS, PVC, polycarbonate, and phenolic materials
  • Rapid assembly of closely fitted parts
Product Family

PERMABOND 105

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
colorless
Chemistry Type
Ethyl cyanoacrylate
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
30-50 mPa.s
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
25 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties and processing characteristics of PERMABOND® 105 before full cure. Values are guideline information and do not constitute a specification.

Property Value Unit Method / condition
Chemical composition Ethyl cyanoacrylate — As supplied
Appearance Colorless — As supplied
Viscosity 30–50 mPa·s (cP) At 25°C
Specific gravity 1.1 — Typical
Maximum gap fill 0.1 (0.004) mm (in) Closely fitted bonded joint
Fixture / handling time 5–20 seconds 0.3 N/mm² shear strength achieved; substrate-dependent
Full-strength time 24 hours Temperature, humidity, substrate, surface acidity, and gap can affect cure speed
Technical properties

After-processing / final-state properties

Typical properties and substrate-specific performance of the cured adhesive. Strength results vary with surface preparation and joint gap and do not constitute specifications.

Property Value Unit Method / condition
Shear strength on steel 18–22 (2,600–3,200) N/mm² (psi) ISO 4587
Shear strength on aluminum 6–8 (900–1,200) N/mm² (psi) ISO 4587
Shear strength on PVC >10 (>1,400) N/mm² (psi) ISO 4587; substrate failure
Shear strength on phenolic 12–14 (1,700–2,000) N/mm² (psi) ISO 4587
Impact strength 3–5 (1.4–2.4) kJ/m² (ft·lb/in²) ASTM D950
Hardness 85 Shore D ISO 868
Dielectric strength 25 kV/mm Typical cured-material property
Thermal conductivity 0.1 W/(m·K) Typical cured-material property