Main features

  • 15-26 Minute Open Time
  • 0.125 in Gap Filling
  • 3,000 psi Steel Shear

Product Description

H.B. Fuller MP-55350 Methacrylate Structural Adhesive is an extended-working-time two-part methyl methacrylate adhesive for structural bonding of metals, thermosets, thermoplastics, and composites. A 1:1 resin-to-activator mix provides a 15-26 minute open time for placement and alignment, followed by fixture in 35-55 minutes at 25 deg C. The material fills gaps up to 0.125 in and reaches full cure in 24 hours. Typical cured properties include Shore D 75 hardness, 3,190-4,640 psi tensile strength, and ASTM D1002 overlap shear of 3,000 psi on carbon steel and 2,800 psi on aluminum.

Key features

  • Extended open time: Provides 15-26 minutes for placement and alignment at 25 deg C.
  • Controlled fixture window: Develops fixture strength in 35-55 minutes at 25 deg C.
  • Structural overlap shear: Reaches 3,000 psi on carbon steel and 2,800 psi on aluminum under ASTM D1002 conditions.

Applications / Suitable for

  • Bonding aluminum, steel, stainless steel, and e-coated metal structures
  • Bonding fiberglass, phenolic, gel coat, epoxy, and polyurethane components
  • Bonding ABS, polycarbonate, nylon/PA, PVC, PEEK, and PBT or PET blends
Product Family

MP 55350

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Methyl Methacrylate
Color
The color
Off white or amber
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
two
Density (g)
0.98 g/cm3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
10 °C
Operating Temperature
-67 to 250 °C

Additional Information

Technical properties

Uncured and working properties

Property Value Unit Method / condition
Mix ratio 1:1 by volume or weight Resin to activator
Resin viscosity 60,000-120,000 cP Brookfield RV7; 20 rpm; 25 deg C
Activator viscosity 60,000-110,000 cP Brookfield RV7; 20 rpm; 25 deg C
Mixed density 0.98 g/cc Typical
Open time 15-26 min 25 deg C
Fixture time 35-55 min 25 deg C
Full cure 24 h Room temperature
Maximum gap fill 0.125 in Bondline
Technical properties

Cured properties

Property Value Unit Method / condition
Shore hardness 75 Shore D ASTM D2240
Tensile strength 3,190-4,640 psi ASTM D638
Overlap shear on carbon steel 3,000 psi ASTM D1002; 25 deg C; 50% RH
Overlap shear on aluminum 2,800 psi ASTM D1002; 25 deg C; 50% RH
Thermal service range -67 to 250 deg F Cured adhesive