MP 55320

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MP 55320

Main features

  • No-Prep Multi-Substrate Bonding
  • 7 to 12-Minute Open Time
  • Thermal-Cycling/Chemical-Resistant Flexible Bonding

Product Description

MP-55320 is a high-performance, two-part modified acrylic structural adhesive engineered for bonding a wide range of plastics, metals, and composites. It cures at room temperature to deliver exceptional flexibility, outstanding bond strength, and robust resistance to extreme temperature fluctuations, thermal cycling, and harsh chemicals.

Key features

  • No surface preparation required: Achieves excellent adhesion and impact resistance to most substrates without the need for prior surface treatment.
  • Extended open time: Offers a 7 to 12 minute open time and 16 to 27 minute fixture time, providing flexibility for complex assemblies.
  • Convenient 10:1 mix ratio: Easily dispensed using manual or pneumatic equipment for consistent meter-mix application.

Applications / Suitable for

  • Engineered for metals including aluminum, steel, stainless steel, and e-coated metal.
  • Ideal for thermosets such as fiberglass, epoxy, phenolic, and polyurethane.
  • Suitable for a wide array of thermoplastics, including acrylic, ABS, polycarbonate, and nylon/PA.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Off-white or amber, viscous liquid
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
10:1
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
8–14 min minutes
Product Type
Material category or functional product class.
Two-part modified acrylic structural adhesive

Additional Information

Technical properties

As-supplied / before-processing properties

Pre-cure properties of MP-55320 structural adhesive.

Property Value Unit Method / condition
Appearance / Color Off-white or Amber - -
Mix Ratio (Volume & Weight) 10:1 - -
Viscosity (Resin) 130,000 - 180,000 cPs Brookfield RV7, 20 RPM, 25°C
Viscosity (Activator) 40,000 - 80,000 cPs Brookfield RV7, 20 RPM, 25°C
Mixed Density 0.95 g/cc -
Open Time 7-12 Minutes -
Fixture Time 16-27 Minutes -
Technical properties

After-processing / final-state properties

Cured mechanical and thermal properties of MP-55320.

Property Value Unit Method / condition
Hardness 45 Shore D ASTM D2240
Tensile Strength 15 to 30 (2175 to 4350) MPa (psi) ASTM D638
Overlap Shear Strength (Carbon Steel) 2900 psi ASTM D1002, 25°C 50% RH
Overlap Shear Strength (Aluminum) 2900 psi ASTM D1002, 25°C 50% RH
Thermal Service Range -67 to 250 °F -