MP 55310

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

MP 55310

Main features

  • 7-9 Minute Open Time
  • 19-23 Minute Fixture Time
  • 3,300 psi Steel Shear

Product Description

H.B. Fuller MP-55310 Methacrylate Structural Adhesive provides a two-part methyl methacrylate system for structural bonding of metals, thermosets, thermoplastics, and composite assemblies. The resin and activator mix 1:1 by volume or weight and provide a 7-9 minute open time with fixture in 19-23 minutes at 25 deg C. The adhesive fills gaps up to 0.125 in and reaches full cure in 24 hours. Typical cured data include Shore D 75 hardness, 4,350-5,800 psi tensile strength, and overlap shear of 3,300 psi on carbon steel and 3,100 psi on aluminum under ASTM D1002 conditions.

Key features

  • Seven-to-nine-minute open time: Provides a defined working window for adhesive placement and assembly.
  • Nineteen-to-twenty-three-minute fixture: Develops fixture strength in 19-23 minutes at 25 deg C.
  • One-eighth-inch gap fill: Fills bond gaps up to 0.125 in in bonded assemblies.

Applications / Suitable for

  • Bonding aluminum, steel, stainless steel, and e-coated metals
  • Bonding fiberglass, phenolic, gel coat, epoxy, and polyurethane materials
  • Bonding ABS, polycarbonate, nylon/PA, PVC, PEEK, and PBT or PET blends
Product Family

MP 55310

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Methyl Methacrylate
Color
The color
Off white or amber
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
two
Density (g)
0.98 g/cm3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
10 °C
Operating Temperature
-67 to 250 °C

Additional Information

Technical properties

Uncured and working properties

Property Value Unit Method / condition
Mix ratio 1:1 by volume or weight Resin to activator
Resin viscosity 60,000-80,000 cP Brookfield RV7; 20 rpm; 25 deg C
Activator viscosity 60,000-110,000 cP Brookfield RV7; 20 rpm; 25 deg C
Mixed density 0.98 g/cc Typical
Open time 7-9 min 25 deg C
Fixture time 19-23 min 25 deg C
Full cure 24 h Room temperature
Maximum gap fill 0.125 in Bondline
Technical properties

Cured properties

Property Value Unit Method / condition
Shore hardness 75 Shore D ASTM D2240
Tensile strength 4,350-5,800 psi ASTM D638
Overlap shear on carbon steel 3,300 psi ASTM D1002; 25 deg C; 50% RH
Overlap shear on aluminum 3,100 psi ASTM D1002; 25 deg C; 50% RH
Thermal service range -67 to 250 deg F Cured adhesive

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers